Patents
US 7,547,643 B2#17185874 Most CitedExpiredUnited States (USPTO)Utility

Techniques promoting adhesion of porous low K film to underlying barrier layer

6Forward Citations (#17185874 Global)
0.3/yrCitation Velocity (#22383796 Global)
1.82Citation PageRank (#16881483 Global)
29Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Adhesion of a porous low K film to an underlying barrier layer is improved by forming an intermediate layer lower in carbon content, and richer in silicon oxide, than the overlying porous low K film. This adhesion layer can be formed utilizing one of a number of techniques, alone or in combination. In one approach, the adhesion layer can be formed by introduction of a rich oxidizing gas such as O 2 /CO 2 /etc. to oxidize Si precursors immediately prior to deposition of the low K material. In another approach, thermally labile chemicals such as alpha-terpinene, cymene, and any other non-oxygen containing organics are removed prior to low K film deposition. In yet another approach, the hardware or processing parameters, such as the manner of introduction of the non-silicon containing component, may be modified to enable formation of an oxide interface prior to low K film deposition. In still another approach, parameters of ebeam treatment such as dosage, energy, or the use of thermal annealing, may be controlled to remove carbon species at the interface between the barrier and the low K film. In a further approach, a pre-treatment plasma may be introduced prior to low k deposition to

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 6.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for promoting adhesion between a nanoporous low K film and an underlying liner/baffler layer, the method comprising: providing a substrate bearing a liner/barrier layer; forming a carbon-containing silicon oxide adhesion layer over the liner/barrier layer by exposing the liner/barrier layer to a rich oxidizing gas that oxidizes Si precursors on an exposed surface of the liner/barrier layer, prior to deposition of a low K film; depositing the low K film over the adhesion layer, wherein the carbon-containing silicon oxide adhesion layer is lower in carbon content, and richer in silicon

  2. Claim 2Depends on #1

    The method of claim 1 wherein providing the substrate comprises providing the substrate bearing a silicon carbide liner/barrier layer.

  3. Claim 3Independent Claim

    The me

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 5,003,113 AProcess of producing isopropylnaphthols19913
US 5,003,178 ALarge-area uniform electron source1991238
US 5,362,526 APlasma-enhanced CVD process using TEOS for depositing silicon oxide1994252
US 5,468,595 AMethod for three-dimensional control of solubility properties of resist layers199598
WO 9,941,423 A2Plasma processes for depositing low dielectric constant films—169
US 6,001,728 AMethod and apparatus for improving film stability of halogen-doped silicon oxide films199933
US 6,051,881 AForming local interconnects in integrated circuits200032
US 6,132,814 AMethod for curing spin-on-glass film utilizing electron beam radiation2000104
US 6,150,070 AMethod of creating optimal profile in single layer photoresist200019
US 6,171,945 B1CVD nanoporous silica low dielectric constant films2001247
US 6,195,246 B1Electrostatic chuck having replaceable dielectric cover200128
US 6,204,201 B1Method of processing films prior to chemical vapor deposition using electron beam processing200174
US 6,207,555 B1Electron beam process during dual damascene processing200169
US 6,218,090 B1Method of creating controlled discontinuity between photoresist and substrate for improving metal lift off200120
US 6,255,035 B1Method of creating optimal photoresist structures used in the manufacture of metal T-gates for high-speed semiconductor devices200180
US 6,271,146 B1Electron beam treatment of fluorinated silicate glass200154
US 6,319,555 B1Metering device for paint for digital printing200119
US 6,319,655 B1Modification of 193 nm sensitive photoresist materials by electron beam exposure200165
US 6,340,556 B1Tailoring of linewidth through electron beam post exposure200225
US 6,351,039 B1Integrated circuit dielectric and method200267
US 6,358,670 B1Enhancement of photoresist plasma etch resistance via electron beam surface cure200276
US 6,407,399 B1Uniformity correction for large area electron source200275
US 6,426,127 B1Electron beam modification of perhydrosilazane spin-on glass200235
US 2003032274 A1Method for eliminating reaction between photoresist and OSG—23