US 7,547,407 B2#6139797 Most CitedExpiredUnited States (USPTO)Utility

Manufacturing method for sintered body with buried metallic member

15Forward Citations (#6139797 Global)
0.9/yrCitation Velocity (#8155750 Global)
3.60Citation PageRank (#5655209 Global)
9Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A manufacturing method for a sintered body having a metallic member buried therein is provided, and includes forming an alumina sintered body, forming a metallic member by printing a printing paste including a refractory metal on the alumina sintered body, forming a green alumina compact on the metallic member, and sintering the alumina compact, the metallic member, and the alumina sintered body or the alumina presintered body.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 15.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A manufacturing method for a sintered body having a metallic member buried therein, comprising: forming an alumina sintered body having a first surface and an opposed second surface; polishing the opposed second surface of the alumina sintered body; forming a metallic member by printing a printing paste including a refractory metal on the polished second surface of the alumina sintered body; forming a green alumina compact on the metallic member; hot pressing the green alumina compact, the metallic member, and the alumina sintered body to sinter the green alumina compact, the metallic member a

  2. Claim 2Independent Claim