Abstract
Making mats using glass fibers having a diameter of about 13+/−3 microns, bound with a binder formed from a homopolymer or a copolymer of polyacrylic acid and a polyol produces fibrous nonwoven mats having high tensile strength and also an unexpected high flame resistance considering the amount of oxygen in the binder. Mats of the present invention pass the National Fire Protection Association's (NFPA) Flammability Test. Tabor stiffness of these mats is greater than about 40, preferably greater than about 50 and most preferably greater than about 55. Air permeability of the mats is preferably within the range of about 500 to about 800 CFM/sq. ft. Methods of making the mat are also disclosed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for making a fibrous nonwoven mat facer suitable as a backer mat, connector sheet, in a compressible ceiling panel of the type described in U.S. Published Patent Application No. 200200020142, filed Apr. 23, 2001, comprising; a) dispersing glass fibers having an average fiber diameter of 13+/−1.5 microns and a length of about 0.75+/−0.15 inch in an aqueous dispersion, b) draining said dispersion through a moving forming screen to form a wet fibrous web, c) applying an aqueous resin binder to the wet web and removing excess binder to produce a binder content in the web, after drying, in
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗