US 7,543,733 B2#27294700 Most CitedExpiredUnited States (USPTO)Utility

Method of protecting against corrosion at high temperature

4Forward Citations (#27294700 Global)
0.2/yrCitation Velocity (#30586172 Global)
1.05Citation PageRank (#38993304 Global)
18Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a method of protecting equipment intended to operate at high temperature in the presence of a fluid containing at least one hydrocarbon and/or carbon monoxide against corrosion by metal dusting, method in which pieces of the equipment are made from an alloy containing nickel, iron, chromium and/or aluminum, and in which said pieces of the equipment are protected from said corrosion by a protective coating. This method is characterized in that said equipment pieces protected in this way are connected to each other by means of joining pieces, said joining pieces being protected beforehand by a protective coating over at least part of their surface intended to be brought into contact with said fluid at high temperature, and in that each of the connections intended to be subjected to said corrosion is produced by external welding of the ends of the joining piece with said pieces of equipment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for protecting a tubular junction, comprising: providing a first tubular and a second tubular, each tubular having an outer surface and an interior surface for the passage of fluid; placing a protective surface finish on an interior of the tubulars; providing a joining tubular having a surface finish on an interior thereof; connecting the joining tubular between the first and second tubulars to create a junction, the junction only including the joining tubular and an end of each of the first and second tubulars and having a continuous surface finish on an interior surface thereof; and

  2. Claim 2Independent Claim

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗