Conjugated-diolefin (co)polymer rubber and process for producing the same
Abstract
A method for producing an alkoxysilyl group-containing conjugated diolefin (co)polymer rubber by polymerizing a conjugated diolefin or a conjugated diolefin and an aromatic vinyl compound in a hydrocarbon solvent by anionic polymerization using as an initiator at least one metal compound selected from an organic alkali metal compound and an organic alkali earth metal compound, and then allowing an alkoxysilane-based compound to react, wherein after the alkoxysilane-based compound has been allowed to react, an alkaline compound is added at the time of desolvation, and treatment is conducted at a pH of 8 to 12.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 11.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for producing an alkoxysilyl group containing conjugated diolefin (co)polymer rubber from a conjugated diolefin or a conjugated diolefin and an aromatic vinyl compound, wherein said (co)polymer rubber has an alkoxysilyl group and has been desolvated under alkaline conditions, comprising polymerizing a conjugated diolefin or a conjugated diolefin and an aromatic vinyl compound in a hydrocarbon solvent by anionic polymerization using as an initiator at least one metal compound selected from the group consisting of an organic alkali metal compound and an organic alkali earth metal compou
- Claim 2Depends on #1
The method according to claim 1
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (2)
- U.S. Appl. No. 10/567,905, filed Feb. 10, 2006, Taniguchi et al.
- U.S. Appl. No. 10/591,279, filed Aug. 31, 2006, Kobayashi et al.