Patents
US 7,524,920 B2#18774269 Most CitedExpiredUnited States (USPTO)Utility

Biaxially oriented copolyester film and laminates thereof

6Forward Citations (#18774269 Global)
0.3/yrCitation Velocity (#22480515 Global)
1.28Citation PageRank (#29092426 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a biaxially-oriented polyester film produced from a polyester comprising: (1) diacid residues comprising between about 95 and about 100 mole percent of terephthalic acid residues; (2) diol residues comprising between about 95 and about 100 mole percent of 1,4-cyclohexanedimethanol residues; and (3) about 0.5 to about 5 mole percent of another dicarboxylic acid or diol residue, wherein the polyester comprises a total of 100 mole percent diacid residues and a total of 100 mole percent diol residues. In one embodiment, the biaxially-oriented film has a thickness of 70 to 150 microns (3-5 mils). In another embodiment, the biaxially-oriented film undergoes not more than 3% shrinkage when immersed for 10 seconds in a solder bath preheated to 260° C. The film can be made by stretching an essentially amorphous cast film of thickness between about 450-1800 micron (18-70 mil) at a ratio from about 2.5×2.5 to 3.5×3.5 while being held at a temperature between 90° C. and 130° C., and heat-setting the stretched film at an actual film temperature of from 260° C. to Tm, where Tm is the melting point of the polyester as measured by differential scanning calorimetry (DSC), while maintai

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A biaxially-oriented polyester film produced from a polyester comprising: (a) diacid residues comprising between about 95 and about 100 mole percent of terephthalic acid residues; (b) diol residues comprising between about 95 and about 100 mole percent of 1,4-cyclohexanedimethanol residues; and (c) about 0.5 to about 5 mole percent of another dicarboxylic acid or diol residue, wherein the polyester comprises a total of 100 mole percent diacid residues and a total of 100 mole percent diol residues, and wherein the polyester film has been heat set at an actual film temperature of from 260° C. to

  2. Claim 2Depends on #1

    The biaxially-oriented polyester film of claim 1 , which is produced by stretching an essentially amorphous cast

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,901,466 ALinear polyesters and polyester-amides from 1,4-cyclohexanedimethanol1959367
US 3,284,223 AMagnetic recording tape supported on terephthalate polyesters of 1, 4-cyclohexanedimethanol19669
GB 1,117,904 AProcess for improving dimensional stability of tensilized polyester film—5
US 3,896,076 AAdhesive composition for flexible printed circuit and method for using the same197523
US 3,907,754 AProcess and catalyst-inhibitor system for preparing synthetic linear polyester1975125
US 3,962,145 AHigh temperature thermistor composition197617
US 3,962,189 AProcess and catalyst-inhibitor systems for preparing synthetic linear polyesters1976170
US 4,010,145 AProcess and catalyst inhibitor systems for preparing synthetic linear polyesters1977167
US 4,356,299 ACatalyst system for a polyethylene terephthalate polycondensation198280
US 4,362,775 APolyester film-heat-bonded metal sheet and container made thereof1982108
JP S58214208 AElectrically insulating film—3
JP S60215 B2二軸延伸ブロ−成形容器の製造法—2
JP S6069133 ABiaxially orientated polyester film—4
JP S6085437 AFlexible disc for magnetic recording—6
US 4,557,982 AMagnetic recording flexible disc198515
JP H01299019 APolyester biaxially oriented film—2
JP H02164632 ACleaning device equipped in—5
JP H02187331 ABase film for flexible printed wiring board—7
JP H02191638 ABiaxially oriented polyester film—14
JP H02196833 AElectrical insulating material and film for metallizing—4
JP H02284929 AWhite polyester film—21
JP H02301419 AHeat resistant biaxially oriented polyester film and manufacture thereof—5
US 5,017,680 AProcess and catalyst-inhibitor systems for preparing poly(ethylene terephthalate)1991156

Non-Patent Literature (5)

  • "Oriented Polyester Film," Research Disclosure, May 1990, p. 368, vol. 313, No. 10, Havant GB.
  • "Poly(1,4-Cyclohoxylenedimethylene 2,6-Naphthalenedicarboxylate) Polymers and Copolymers Containing Aromatic Acids", Research Disclosure, Oct. 1988, pp. 798-805.
  • Copending U.S. Appl. No. 10/606,070 filed Jun. 25, 2003, Pecorini et al.
  • Copending U.S. Appl. No. 11/431,238, filed May 10, 2006, Pecorini et al.
  • Copending U.S. Appl. No. 11/803,025, filed May 11, 2007, Thomas Joseph Pecorini et al.