Disclosed herein is a manufacturing method of a planar resistance heating element and a planar resistance heating element made using the method. In the manufacturing method of a planar resistance heating element by etching an aluminum foil deposited on an insulating substrate in a desired pattern, printing carbon paste and connecting current input terminals in parallel, the aluminum foil is adapted to undergo a multiple step tempering process to thereby prevent heat deformation. The carbon paste acting as a resistor element is made of electrically conductive carbon, graphite, a resin, a solvent and a hardener which are mixed so as to optimize physical properties of the carbon paste. As a result, prevention of heat deformation of the insulating substrate, uniform heat conductivity, excellent heat-generation effect and easy manufacture may be achieved. In addition, the use of the carbon paste having optimized physical properties as a resistor element results in good heat-generation and near-zero temperature variation.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a planar resistance heating element, said method comprising: a) tempering an aluminum foil deposited on an insulating substrate in a stepwise manner at a temperature of 0 to 40 degree C. for 1.5 to 2.5 hours, thereafter at a temperature of 40 to 70 degree C. for 1.5 to 2.5 hours, thereafter at a temperature of 70 to 100 degree C. for 2.5 to 3.5 hours, and thereafter at a temperature of 100 to 130 degree C. for 14 to 18 hours; b) then etching said aluminum foil in a desired pattern to make a planar resistance heating element; and c) then printing carbon paste and conn

  2. Claim 2Depends on #1

    The manufacturing method of claim 1 , wherein the tempered aluminum foil is cleaned using a cleansing solution of pH 10 to 12, and dried at a temperature of 50 to 65° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.