US 7,517,827 B2#5010467 Most CitedActiveUnited States (USPTO)Utility

Process for preparation of liquefied petroleum gas selective cracking catalyst

18Forward Citations (#5010467 Global)
1.1/yrCitation Velocity (#6063210 Global)
2.43Citation PageRank (#10663426 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a cracking catalyst composition for cracking heavy hydrocarbon and processes for preparing the catalyst. The process can include treating zeolite with sodium free basic compound with or without phosphate, treating an alumina with a dilute acid, acidifying a colloidal silica, preparing a fine slurry of clay with a source of phosphate, adding alumina slurry and/or acidified colloidal silica to clay phosphate slurry, adding treated zeolite and spray-drying the slurry and calcining the same to obtain a cracking catalyst having adequate ABD and attrition resistance property.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a catalyst composition for cracking heavy hydrocarbon, comprising: treating a high silica low soda medium pore zeolite with an ammoniacal solution to obtain a zeolite slurry having a pH between about 5 to about 9; treating an alumina with a dilute acid to obtain an alumina binder; preparing an acidic clay slurry with a source of phosphate; combining the treated zeolite, the alumina binder, and the clay slurry, to obtain a slurry mixture; and spray-drying and calcining the slurry mixture to obtain the catalyst.

  2. Claim 2Depends on #1

    The process of claim 1 , wherein the zeolite includes at least one of ZSM-5, ZSM-11, ZSM-12, ZSM-23, ZSM-35, ZSM-38, ZSM-48, ZSM-57, Zeolite beta, and mordenite.

  3. Claim 3Depends on #1

    The process of claim 1 , wherein the alumina is selected from a group consisting of pseudoboehmite alumina, boehmite, aluminum trihydrat

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 10,413,889 B2Composition and process for preparation of cracking catalyst suitable for enhancing yields of light olefins20190
US 2022410127 A1Method for preparing a catalyst support—0
US 12,350,649 B2Method for preparing a catalyst support20250
EP 3,135,373 A1Preparation and composition of a fluid catalytic cracking catalyst additive with lower phosphate content for enhanced lpg yield—2
US 10,449,524 B2Process and composition for preparation of cracking catalyst suitable for enhancing LPG20190
EP 2,548,644 A1FCC catalyst additive and a method for its preparation—10
EP 3,135,748 A1A composition and a process for preparation of attrition resistant cracking catalyst suitable for enhancing light olefins—1
US 11,427,764 B2FCC catalyst with more than one silica, its preparation and use20220
US 2013023710 A1Fcc catalyst additive and a method for its preparation—20
WO 2014/015302 A1Catalysts for thermo-catalytic conversion of biomass, and methods of making and using—2
US 10,384,948 B2Cracking catalyst composition for cracking of heavy hydrocarbon feed stocks and process for preparing the same20190
US 10,252,249 B2Composition and a process for preparation of attrition resistant cracking catalyst suitable for enhancing light olefins20190
CN 104,602,813 ACatalysts for thermo-catalytic conversion of biomass, and methods of making and using—0
US 10,245,581 B2Composition and process for preparation of attrition resistant additive suitable for cracking hydrocarbon feed20190
US 9,067,196 B2FCC catalyst additive and a method for its preparation20156