Catalysts with high cobalt surface area
Abstract
A method of making a cobalt-containing catalyst precursor, comprising slurrying a transition alumina powder with an aqueous solution of a cobalt ammine complex, heating the slurry to cause the cobalt ammine complex to decompose with the deposition of an insoluble cobalt compound, filtering the solid residue from the aqueous medium, and drying the solid residue.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of making a catalyst precursor containing 20 to 85% by weight of total cobalt, comprising: slurrying a transition alumina powder having a pore volume above 0.7 ml/g with an aqueous solution of a cobalt ammine complex, heating the slurry to cause the cobalt ammine complex to decompose with the deposition of an insoluble cobalt compound, filtering the solid residue from the aqueous medium, and drying the solid residue.
- Claim 2Depends on #1
A method according to claim 1 wherein the slurry is heated for a period of not more than 200 minutes to cause the cobalt ammine complex to decompose.
- Claim 3Depends on #1
A method according to claim 1 wherein the transition alumina powder has a surface-weighted mean diameter D[3,2] in the range 1 μm to 200 μm.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 11,376,567 B2 | Methods for preparing catalytic systems | 2022 | 0 |