Patents
US 7,501,355 B2#2698323 Most CitedActiveUnited States (USPTO)Utility

Decreasing the etch rate of silicon nitride by carbon addition

27Forward Citations (#2698323 Global)
1.6/yrCitation Velocity (#3173335 Global)
3.93Citation PageRank (#4896911 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Methods for forming silicon nitride hard masks are provided. The silicon nitride hard masks include carbon-doped silicon nitride layers and undoped silicon nitride layers. Carbon-doped silicon nitride layers that are deposited from a mixture comprising a carbon source compound, a silicon source compound, and a nitrogen source in the presence of RF power are provided. Also provided are methods of UV post-treating silicon nitride layers to provide silicon nitride hard masks. The carbon-doped silicon nitride layers and UV post-treated silicon nitride layers have desirable wet etch rates and dry etch rates for hard mask layers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 27.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a silicon nitride hard mask, comprising: introducing a silicon source compound into the chamber; introducing a nitrogen source into the chamber; reacting the silicon source compound and nitrogen source in the presence of RF power to deposit a silicon nitride layer on a substrate in the chamber; and reducing a wet etch rate of the silicon nitride layer by UV post-treating the silicon nitride layer to form the silicon nitride hard mask.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the silicon source compound is silane, trimethylsilane, or TEOS and the nitrogen source is NH 3 .

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the substrate is maintained at a temperature between about 480° C. and about 600° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 27 total)

PatentTitleYearCitations
US 12,225,725 B2Semiconductor devices and manufacturing methods of the same20250
US 8,772,102 B2Methods of forming self-aligned contacts for a semiconductor device formed using replacement gate techniques201411
US 2009274852 A1Method for fabricating high compressive stress film and strained-silicon transistors—0
US 2016365315 A1Semiconductor structure and process thereof—4
US 8,586,487 B2Low temperature plasma enhanced chemical vapor deposition of conformal silicon carbon nitride and silicon nitride films20137
US 9,646,818 B2Method of forming planar carbon layer by applying plasma power to a combination of hydrocarbon precursor and hydrogen-containing precursor20170
US 10,186,453 B2Semiconductor structure and process thereof20190
US 12,451,434 B2Methods of forming microelectronic devices including differently sized conductive contact structures20250
US 12,347,677 B2Enhanced ignition in inductively coupled plasmas for workpiece processing20250
US 8,741,723 B2Methods of forming self-aligned contacts for a semiconductor device201424
US 7,732,324 B2Semiconductor device having improved adhesion and reduced blistering between etch stop layer and dielectric layer20101
US 9,748,093 B2Pulsed nitride encapsulation20171
US 11,848,204 B2Enhanced ignition in inductively coupled plasmas for workpiece processing20230
US 2009160059 A1Semiconductor Device Having Improved Adhesion and Reduced Blistering Between Etch Stop Layer and Dielectric Layer—0
US 9,378,943 B2Method of manufacturing semiconductor device, method of processing substrate substrate processing apparatus and non-transitory computer-readable recording medium20160

Non-Patent Literature (5)

  • George, et al "Surface Chemistry for Atomic Layer Growth", J.Phys. Chem. 1996, vol. 100, No. 31, pp. 13121-13131.
  • International Search Report dated Apr. 11, 2005 for International Publication No. PCT/US2004/027584.
  • Lee, et al. "Cyclic technique for the enhancement of highly oriented diamond film growth", Thin Solid Films 303 (1997) pp. 264-268.
  • Min, et al. "Chemical Vapor Deposition of Ti-Si-N Films with Alternating Source Supply", Mat. Res. Soc. Symp. Proc. 1999, vol. 564, pp. 207-211.
  • Min., et al. "Metal-organic atomic-layer deposition of titanium-silicon-nitride films", Appl. Phys. Lett., vol. 75 No. 11, 1999, pp. 1521-1523.