Oilwell sealant compositions comprising alkali swellable latex
Abstract
Sealant compositions comprising an alkali swellable latex and a pH increasing material and methods of using the same to service a wellbore are provided. In one embodiment, the sealant composition can be used in a wellbore and includes an alkali swellable latex and a pH increasing material. The sealant composition can have a pH of from about 7 to about 14. In other embodiments, the pH increasing material includes a base-producing material. The base-producing material can include alkali and alkali earth metal carbonates, alkali and alkali earth metal bicarbonates, alkali and alkali earth metal hydroxides, alkali and alkali earth metal oxides, alkali and alkali earth metal phosphates, alkali and alkali earth metal hydrogen phosphates, alkali and alkaline earth metal sulphides, alkali and alkaline earth metal salts of silicates, alkali and alkaline earth metal salts of aluminates, water soluble or water dispersible organic amines, polymeric amine, amino alcohols, or combinations thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 37.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of servicing a wellbore in contact with a subterranean formation, comprising: (A) separately introducing an alkali swellable latex and a pH increasing material to a wellbore; and (B) contacting the alkali swellable latex with the pH increasing material to form a sealant composition in situ within the wellbore, wherein the sealant composition further comprises a non-alkali swellable latex.
- Claim 2Depends on #1
The method of claim 1 , wherein a sufficient amount of the pH increasing material is contacted with the alkali swellable latex to provide the sealant composition having a pH of from about 7 to about 14.
- Claim 3Depends on #1
The method of claim 1 , wherein a sufficient amount of the pH increasing material is contacted with the alkali swellable latex to provide the sealant composition having a pH of from about 8 to about 13.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 37 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Advisory Action dated Apr. 12, 2007 (2 pages), U.S. Appl. No. 11/827,022, filed on Apr. 19, 2004.
- Advisory Action dated Dec. 14, 2007 (3pages), U.S. Appl. No. 10/827,022, filed on Apr. 19, 2004.
- Advisory Action dated Mar. 19, 2007 (3 pages), U.S. Appl. No. 11/827,022, filed on Apr. 19, 2004.
- Baroid borchure entitled "SteelSeal Fine(TM) Lost Circulation Material" dated 2002.
- Baroid borchure entitled “SteelSeal Fine™ Lost Circulation Material” dated 2002.