Highly doped III-nitride semiconductors
Abstract
A method of forming a highly doped layer of AlGaN, is practiced by first removing contaminants from a MBE machine. Wafers are then outgassed in the machine at very low pressures. A nitride is then formed on the wafer and an AlN layer is grown. The highly doped GaAlN layer is then formed having electron densities beyond 1×10 20 cm −3 at Al mole fractions up to 65% are obtained. These levels of doping application of n-type bulk, and n/p tunnel injection to short wavelength UV emitters. Some applications include light emitting diodes having wavelengths between approximately 254 and 290 nm for use in fluorescent light bulbs, hazardous materials detection, water purification and other decontamination environments. Lasers formed using the highly doped layers are useful in high-density storage applications or telecommunications applications. In yet a further embodiment, a transistor is formed utilizing the highly doped layer as a channel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 3.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of doping AlGaN, the method comprising: removing contaminants from a MBE machine; outgassing a wafer in the MBE machine at low pressure; forming a nitride on the wafer; growing an AlN layer by opening Al and RF shutters at a first Al temperature; lowering the Al temperature for a period of time during such AlN layer growth; and growing a doped AlGaN layer by opening RF, Al, Ga and dopant shutters, wherein the AlGaN layer has a doping density beyond degeneracy.
- Claim 2Independent Claim
A method of doping AlGaN, the method comprising: removing contaminants from a MBE machine; outgassing a wafer in the MBE machine at low pressure at a temperature raised to approximately 400 C and lowered over approximately an hour; forming a nitride on the wafer; growing an AlN layer by opening Al and RF shutters for a period of time with the Al temperature at approximately 1276 C;
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (20)
Non-Patent Literature (5)
- "Essentials of the Free Electron Gas", Semiconductor Physics, http://www.techfak.uni-kiel.de/matwis/amat/semi-en/kap-backbone/r2-1-1.html,(2002),60 pages.
- "U.S. Appl. No. 10/140,774 Final office action mailed Dec. 2, 2003", 11 pgs.
- "U.S. Appl. No. 10/140,774 Non Final office action mailed Apr. 5, 2004", 9 pgs.
- "U.S. Appl. No. 10/140,774 Non Final office action mailed Jun. 20, 2003", 8 pgs.
- "U.S. Appl. No. 10/140,774 Notice of allowance mailed Nov. 19, 2004", 9 pgs.