hottub.patents
US 7,479,185 B2#672016 Most CitedExpiredUnited States (USPTO)Utility

Reflective crack relief layer that is permeable

0Forward Citations (#672016 Global)
0.0/yrCitation Velocity (#672016 Global)
0.97Citation PageRank (#672016 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A design method for making a bituminous mixture that is used to form a vapor-permeable layer of pavement is provided. This design procedure includes preparing one or more bituminous mixture test specimens, measuring the performance of these specimens, and selecting a desirable bituminous mixture for paving that is vapor-permeable based on the performance of the specimens. Another aspect of the present invention is the selected bituminous mixture, which includes aggregate and a bituminous binder. The aggregate should be selected such that no more than about 5% by mass of the aggregate and preferably no more than about 3.5% by mass of the aggregate is able to pass through a 75 μm sieve. The selected bituminous mixture should have an Air Permeability Value that is at least about 8 cm 2 so as to reduce its propensity for blistering during and after construction. Still further, the selected bituminous mixture should have desirable fatigue resistance and should be substantially water-impermeable.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A bituminous mixture comprising: a mixture formed by mixing aggregate and a bituminous binder, said aggregate having no more than 5% passing through a 75 μm screen and at least 70% passing through a 2.36 mm screen, said binder being at least 7% of the mixture, and said mixture having a dust to asphalt ratio of less than 09.

  2. Claim 2Depends on #1

    The bituminous mixture of claim 1 wherein said bituminous mixture has an Air Permeability Value that is at least 8 cm 2 .

  3. Claim 3Depends on #1

    The bituminous mixture of claim 1 wherein said bituminous mixture has an Air Permeability Value that is at least about 10 cm 2 .

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (3)

PatentTitleYearCitations

Non-Patent Literature (3)

  • ASTM Designation D 3637-84 (Reapproved 1991); Standard Test Methods for Permeability of Bituminous Mixtures; pp. 364-369.
  • J.J.E. Liebenberg et al: Asphalt Mix Design and Construction: A Selection of Possible Pitfalls; (Sep. 16, 2004), pp. 1-12; XP002389166; Sun City, South Africa; http://asac.csir.co.za/capsa/Documents/035.pdf.
  • Standard Practice for Superpave Volumetric Design For Hot-Mix Asphalt (HMA); AASHTO Designation: R 35-04; pp. R 35-1 through R 35-13.