A dielectric paste of the present invention contains a binder resin, a cross-linking agent, a thermal polymerization initiator, and an inorganic powder, wherein the content of the thermal polymerization initiator is 3 to 30 parts by weight to 100 parts by weight of the total of the binder resin and the cross-linking agent. A method of manufacturing a plasma display, of the present invention, includes a first step of forming electrode patterns using an electrode paste, a second step of forming a dielectric paste coating film using a dielectric paste, a third step of forming barrier rib patterns using a barrier rib paste, a subsequent step of simultaneously firing at least the electrode patterns, the dielectric paste coating film, and the barrier rib patterns, and a step of performing curing after the second step. The present invention provides a method of manufacturing a plasma display, in which the electrode patterns, the dielectric paste coating film, and the barrier rib patterns can be simultaneously fired without any defects such as disconnections or cracks.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A dielectric paste comprising: a binder resin; a cross-linking agent; a thermal polymerization initiator; and an inorganic powder; wherein the content of the thermal polymerization initiator is in the range of from 3 to 30 parts by weight to 100 parts by weight of the total of the binder resin and the cross-linking agent; and wherein the inorganic powder comprises a glass powder having a softening point of 450 to 600° C. and, to 100 parts by weight of the total of the binder resin and the cross-linking agent, the content of the glass powder is 150 to 300 by weight.

  2. Claim 2Depends on #1

    A dielectric paste according to claim 1 , wherein the thermal polymerization initiator has an initiator efficiency in the range of from 0.8 to 1.0.

  3. Claim 3Depends on #1, #2

    A dielectric paste according to claim 1 or 2 , wherein the thermal polymerizati