US 7,465,769 B2#8612865 Most CitedActiveUnited States (USPTO)Utility

Nitroxide compounds for minimizing scorch in crosslinkable compositions

12Forward Citations (#8612865 Global)
0.7/yrCitation Velocity (#11382764 Global)
1.90Citation PageRank (#15802608 Global)
18Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Scorch is inhibited during the free-radical crosslinking of a crosslinkable polymer, e.g., an EPDM, by incorporating into the polymer before melt processing and crosslinking a scorch inhibiting amount of a derivative, preferably an ether, ester or urethane derivative, of a TEMPO compound, e.g., 4-hydroxy-tetrahydrocarbylpiperidin-1-oxyl. The scorch inhibitors of this invention perform as well, if not better, than their 4-hydroxy-tetrahydrocarbylpiperidin-1-oxyl counterparts in similar polymer compositions and under similar conditions in terms of scorch inhibition and ultimate degree of crosslinking, but exhibit less volatility and less migration within the polymer composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 12.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A polymer composition comprising a (i) free radical initiator, (ii) crosslinkable polymer, and (iii) scorch-inhibiting amount of a TEMPO scorch inhibitor that is at least one of methyl ether TEMPO, butyl ether TEMPO, hexyl ether TEMPO, allyl ether TEMPO and stearyl urethane TEMPO.

  2. Claim 2Depends on #1

    The composition of claim 1 in which the TEMPO compound comprises at least about 0.01 wt % of the composition.

  3. Claim 3Depends on #2

    The composition of claim 2 in which the free radical initiator is at least one of a peroxide or azo compound.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
US 3,202,648 AScorch-resistant polyethylene compositions and method196540
US 3,335,124 ARate-controlled vulcanization of polyethylene196747
US 3,751,378 AInhibiting prevulcanization of rubber with polyfunctional methacrylate monomers as cross-linking coagents with peroxides197382
US 3,862,107 AMethod of curing polymers with azo compounds197535
US 3,954,907 AComposition with selected vinyl compounds and process for avoiding scorching of ethylene polymer composition197670
GB 1,535,039 ACompositions with dicumyl peroxide and process for avoiding scorching of ethylene polymer composition—27
US 4,129,531 ACrosslinking of polymers with azo-esters197848
US 4,632,950 AScorch resistant, crosslinkable composition containing mixture of copper and metal dithiocarbamates198641
US 6,197,213 B1Scorch extending curing/crosslinking compositions20019
US 6,555,019 B2Sulfur free, low color generating scorch time extending compositions for use in compounding and cure of free radical initiator curable polymers20038
US 6,653,409 B2Radical-modified polymer and polymer composition containing the same200314
US 2004138081 A1Organic peroxide heat stabiliser—5
US 6,765,058 B1Scorch extending curing/crosslinking compositions20048
EP 1,322,696 B1Composition comprising a nitroxide, a promoter and optionally a free radical initiator20043
WO 2005/063896 A2Free-radical-initiated crosslinking of polymers—17
WO 2005/066282 A2Rheology modification of polymers—7
WO 2005/066280 A2Free-radical crosslinkable polymers: improved process for crosslinking and compositions—13
US 2005197457 A1Stable organic free radical polymer systems: grafting functional monomers—13