Manufacturing method of thin film integrated circuit device and manufacturing method of non-contact type thin film integrated circuit device
Abstract
With non-contact and contact IC chips becoming common, it is necessary to mass-produce enormous amount of IC chips, which are utilizable for human beings, animals and plants, commercial products, banknotes, and the like, at low cost. For example, it is necessary to manufacture IC chips to be applied to commercial products, banknotes, and the like at a cost of 1 to several yen per IC chip, preferably, at a cost less than 1 yen, and it is desired to realize a structure of an IC chip that can be mass-produced at low cost and a manufacturing process of the IC chip. A method of manufacturing a thin film integrated circuit device according to the present invention includes steps of forming a peel-off layer over a thermally oxidized silicon substrate, forming a plurality of thin film integrated circuit devices over the peel-off layer with a base film interposed therebetween, forming a groove between the plurality of thin film integrated circuit devices, and separating the plurality of thin film integrated circuit devices by introducing one of a gas and a liquid including halogen fluoride into the groove to remove the peel-off layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 10.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of manufacturing a thin film integrated circuit device comprising: forming a plurality of thin film integrated circuit devices on a SOI substrate including an upper single-crystal silicon layer, a layer including one of silicon oxide and silicon nitride, and a lower single-crystal silicon layer; forming a groove in a boundary region between the plurality of thin film integrated circuit devices; and separating the plurality of thin film integrated circuit devices by introducing one of a gas and a liquid including halogen fluoride into the groove to etch at least a surface of the lower
- Claim 2Depends on #1
The method according to claim 1 , wherein the groove is formed by one of linear laser scribing, dicing, and etching with an insulating film as a mask.
- Claim 3Independent Claim
The method accor
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- "Sense of Crisis" is a Trigger: Ignited Evolution of a Sesame-Grain Sized Chip, Nikkei Electronics, Nov. 18, 2002, p. 67-76.
- Search Report of Mar. 15, 2005, European Patent Office for PCT/JP2004/018978.
- Search Report of Mar. 22, 2005, European Patent Office for PCT/JP2005/001541.
- T. Shimoda et al., Surface Free Technology by Laser Annealing (SUFTLA), IEDM 99: Technical Digest of Intrenational Electron Devices Meeting, 1999, pp. 289-292.
- Written Opinion of Mar. 15, 2005, European Patent Office for PCT/JP2004/018978.