Metal/semiconductor/metal (MSM) back-to-back Schottky diode
Abstract
A method is provided for forming a metal/semiconductor/metal (MSM) back-to-back Schottky diode from a silicon (Si) semiconductor. The method deposits a Si semiconductor layer between a bottom electrode and a top electrode, and forms a MSM diode having a threshold voltage, breakdown voltage, and on/off current ratio. The method is able to modify the threshold voltage, breakdown voltage, and on/off current ratio of the MSM diode in response to controlling the Si semiconductor layer thickness. Generally, both the threshold and breakdown voltage are increased in response to increasing the Si thickness. With respect to the on/off current ratio, there is an optimal thickness. The method is able to form an amorphous Si (a-Si) and polycrystalline Si (polySi) semiconductor layer using either chemical vapor deposition (CVD) or DC sputtering. The Si semiconductor can be doped with a Group V donor material, which decreases the threshold voltage and increases the breakdown voltage.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 49.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for forming a metal/semiconductor/metal(MSM) back-to-back Schottky diode from a silicon (Si) semiconductor, the method comprising: depositing an amorphous Si (a-Si) semiconductor layer between a bottom electrode and a top electrode with a DC sputtering process as follows: using a Si target; sputtering with a power in the range of about 100 to 300 watts (W); heating a substrate to a temperature of about 20° to 200° C.; creating a deposition pressure in the range of about 7.0 to 9 mtorr; using an atmosphere of Ar; depositing for a duration in the range of about 7 to 150 minutes; and, fo
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗