Patents
US 7,439,306 B2#17767401 Most CitedExpiredUnited States (USPTO)Utility

Polyethylene blends with improved Vicat softening point

6Forward Citations (#17767401 Global)
0.3/yrCitation Velocity (#22834027 Global)
1.61Citation PageRank (#20464041 Global)
9Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of selecting polyethylene components for a polyethylene composition having an improved Vicat softening point comprising blending at least a first polyethylene having a first density and a second polyethylene having a second density to form the polyethylene composition, wherein the first density is greater than the second density, and determining a first Vicat softening point (V 1 ) of the composition measured, and calculating a second Vicat softening point (V 2 ) of the composition using the formula V 2 =[Σ n 1 {W 1 (Vicat softening point of the first polyethylene)+W 2 (Vicat softening point of the second polyethylene) . . . W n (Vicat softening point of the nth polyethylene)}], wherein W 1 is the weight fraction of the first polyethylene, W 2 is the weight fraction of the second polyethylene and W n is the weight fraction of the nth polyethylene, n ranges from 2 to 10 and W 1 +W 2 . . . +W n =1.0; comparing V 1 and V 2 ; selecting the polyethylene components such that V 1 is less than V 2 for the polyethylene composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 6.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a polyethylene composition, comprising: blending at least a first polyethylene component having a first density and first Vicat softening point and a second polyethylene component having a second density and second Vicat softening point, wherein: the first density is greater than or equal to 0.910 g/cc and the second density is less than 0.910 g/cc; a difference between the first density and the second density ranges from about 0.01 g/cc to about 0.11 g/cc; the polyethylene components are blended in an amount sufficient to provide a Vicat softening point of the blend com

  2. Claim 2Independent Claim

    The metho

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • U.S. Appl. No. 10/803,318, filed Mar. 18, 2004, Ravel et al.