Patents
US 7,438,839 B2#13837191 Most CitedExpiredUnited States (USPTO)Utility

Formulation for the manufacture of carbon-carbon composite materials

8Forward Citations (#13837191 Global)
0.4/yrCitation Velocity (#18329146 Global)
1.55Citation PageRank (#21710313 Global)
20Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Method for manufacturing a carbonized carbon-carbon composite preform, by: mixing (a) chopped carbon fiber, chopped stabilized pitch fiber, or chopped oxidized polyacrylonitrile (PAN) fiber, (b) thermoplastic pitch binder powder, and (c) activated carbon powder to form a mixture of 15-60 parts by weight of chopped carbon fiber or chopped stabilized pitch fiber or chopped oxidized PAN, 28-83 parts by weight of thermoplastic pitch binder powder, and 1-12 parts by weight of activated carbon powder; depositing this mixture into a mold; pressing/heating the materials in the mold to form a preform by compaction; removing the compacted preform from the mold; and carbonizing the compacted preform. The preform is preferably configured in the form of an aircraft landing system brake disc.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a carbonized carbon-carbon composite preform, comprising the steps of: (i) mixing (a) chopped carbon fiber, chopped stabilized pitch fiber, or chopped oxidized polyacrylonitrile (PAN) fiber, (b) thermoplastic pitch binder powder, and (c) activated carbon powder to form a mixture of 15-60 parts by weight of chopped carbon fiber or chopped stabilized pitch fiber or chopped oxidized PAN, 28-83 parts by weight of thermoplastic pitch binder powder, and 1-12 parts by weight of activated carbon powder; (ii) depositing said mixture into a mold; (iii) compression molding the

  2. Claim 2Depends on #1

    The method of claim 1 , wherei

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 4,041,116 AMethod for the manufacture of carbon-carbon composites197733
US 4,451,590 AOrganic friction material198437
US 4,687,607 AProcess for producing electrode substrate for use in fuel cells198720
US 4,959,139 ABinder pitch and method of preparation199021
US 5,395,864 AWet frictional material containing activated carbon fiber199521
US 5,468,357 ADensification of porous articles by plasma enhanced chemical vapor infiltration19959
US 5,776,633 ACarbon/carbon composite materials and use thereof in electrochemical cells199872
US 5,989,390 AFriction paper containing activated carbon199943
US 6,093,482 ACarbon-carbon composite for friction products and method of making same200034
US 6,129,868 AFast process for the production of fiber preforms200023
US 2002170787 A1Wear resistance in carbon fiber friction materials—21
EP 1,323,685 A2Method of production of shaped bodies out of fibre reinforced ceramic materials—4
US 6,699,427 B2Manufacture of carbon/carbon composites by hot pressing200442
US 2004074075 A1Wear resistance in carbon fiber friction materials—19
US 6,749,937 B2Melt-infiltrated pitch-pan preforms200417
US 6,878,331 B2Manufacture of carbon composites by hot pressing200535
US 2005179152 A1Process for producing shaped bodies comprising fiber-reinforced ceramic materials—18
WO 2005/102962 A1Titanium carbide as a friction and wear modifier in friction materials—5
US 2006247121 A1Manufacturing method of activated carbon structure having a frame—5
US 7,207,424 B2Manufacture of carbon/carbon composites by hot pressing200714