US 7,438,769 B2#10210458 Most CitedActiveUnited States (USPTO)Utility

Process for diffusing titanium and nitride into a material having a coating thereon

10Forward Citations (#10210458 Global)
0.6/yrCitation Velocity (#14224818 Global)
2.40Citation PageRank (#10876537 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for diffusing titanium and nitride into a base material having a coating thereon using conventional surface treatments or coatings. The method generally includes the steps of providing a base material having a coating thereon; providing a salt bath which includes sodium dioxide and a salt selected from the group consisting of sodium cyanate and potassium cyanate; dispersing metallic titanium formed by electrolysis of a titanium compound in the bath; heating the salt bath to a temperature ranging from about 430° C. to about 670° C.; and soaking the base material in the salt bath for a time of from about 10 minutes to about 24 hours. In accordance with another aspect of the present invention, titanium and nitride may be diffused into a base material without a coating. The treated base material may further be treated with conventional surface treatments or coatings.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for diffusing titanium and nitride into a base material comprising: providing a base material having a coating thereon, wherein said base material includes a microstructure including voids and said coating has a microstructure including voids contained therein; providing a salt bath which includes sodium dioxide and a salt selected from the group consisting of sodium cyanate and potassium cyanate; dispersing metallic titanium formed by electrolysis of a titanium compound, in said bath; heating the salt bath to a temperature ranging from about 430° C. to about 670° C.; and soaking the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗