Patents
US 7,432,176 B2#149531164 Most CitedExpiredUnited States (USPTO)Utility

Method of three-dimensional microfabrication and high-density three-dimentional fine structure

0Forward Citations (#149531164 Global)
0.0/yrCitation Velocity (#149531164 Global)
0.56Citation PageRank (#149531164 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Surface of a thin film formed on a surface of substrate of Al x Ga y In 1-x-y As z P 1-z (0≦x<1, 0≦y and z≦1) including substances GaAs and InP is irradiated with electron beams controlled at any arbitrary electron beam diameter and current density so as to cause any natural oxide film formed on GaAs surface to undergo selective Ga 2 O 3 substitution or formation. Thereafter, the temperature of the substrate is adjusted to given temperature so as to effect detachment of the natural oxide film at region other than that of Ga 2 O 3 substitution. Selective growth of a Group III-V compound semiconductor crystal is carried out on the substrate on its side of natural oxide film detachment in accordance with the molecular beam epitaxial growing technique to thereby achieve an increase of substrate density. On-site formation of a circuit pattern having the crystal film thickness along the direction of crystal growth uniformalized on the order of nanometers is accomplished.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A three-dimensional very fine patterning method comprising the steps of: preparing a substrate of a Group III-V compound semiconductor including Al x Ga y In 1-x-y As z P 1-z (0≦x<1, 0≦y, z≦1); throwing on the substrate surface an electron beam whose current density is controlled in respect of the diameter of the beam, thereby selectively substituting a Group III oxide for the natural oxide formed on the substrate surface or selectively forming a Group III oxide; raising the temperature of the substrate to a predetermined temperature to allow the parts other than those substituted for or f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.