Patents
US 7,425,299 B2#27210396 Most CitedExpiredUnited States (USPTO)Utility

Lead-free solder balls and method for the production thereof

4Forward Citations (#27210396 Global)
0.2/yrCitation Velocity (#31501866 Global)
1.08Citation PageRank (#37654390 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Lead-free solder balls having a good surface appearance with no appreciable surface defects such as seams and shrinkage cavities comprises an alloy having a composition consisting essentially of about 4.0% to about 6.0% by weight of Ag, about 1.0% to about 2.0% by weight of Cu, and a balance of Sn, and they have a diameter of from 0.05 mm to 1.0 mm. The solder balls can be produced by forming a molten alloy having the above-described composition into solidified balls having a diameter of from 0.05 mm to 1.0 mm using the surface tension of the molten alloy.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Lead-free solder balls for forming solder bumps on a substrate, the composition of the solder balls consisting of 4.0% to 6.0% by weight of Ag, 1.0% to 2.0% by weight of Cu, and a balance of Sn, the solder balls having a diameter of from about 0.05 mm to about 1.0 mm.

  2. Claim 2Depends on #1

    The lead-free solder balls of claim 1 wherein the composition of the solder balls consists of 5.7% by weight of Ag, 1.3% by weight of Cu, and a balance of Sn.

  3. Claim 3Depends on #1

    The lead-free solder balls of claim 1 wherein the solder balls have a good surface appearance which is substantially free of surface defects which may interfere with the use of the solder balls.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗