Metal additives to hydrocarbon feed streams give improved hydrocarbon liquid yield during thermal cracking thereof. Suitable additives include metal overbases and metal dispersions and the metals suitable include, but are not necessarily limited to, magnesium, calcium, aluminum, zinc, silicon, barium, cerium, and strontium overbases and dispersions. Coker feedstocks are a particular hydrocarbon feed stream to which the method can be advantageously applied, but the technique may be used on any hydrocarbon feed that is thermally cracked.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for improving liquid yield during thermal cracking of a refinery hydrocarbon comprising: introducing a metal additive and a dispersant to a refinery hydrocarbon feed stream, where the metal additive is selected from the group consisting of a metal overbase and a metal dispersion, where the metal in the metal additive is selected from the group consisting of aluminum alone, and aluminum and magnesium together; heating the refinery hydrocarbon feed stream to a thermal cracking temperature; and recovering a hydrocarbon liquid product.

  2. Claim 2Depends on #1

    The method of claim 1 where the metal additive contains at least about 1 wt % metal.

  3. Claim 3Depends on #1

    The method of claim 1 where the thermal cracking temperature is between about 850° F. (454° F.) and about 1300° F. (704° C.).

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 3,948,759 AVisbreaking a heavy hydrocarbon feedstock in a regenerable molten medium in the presence of hydrogen1976145
US 4,046,670 AMethod for the treatment of heavy petroleum oil197729
US 4,163,728 APreparation of magnesium-containing dispersions from magnesium carboxylates at low carboxylate stoichiometry197943
US 4,312,745 ANon-puffing petroleum coke198239
US 4,399,024 AMethod for treating petroleum heavy oil198370
US 4,404,092 ADelayed coking process198334
US 4,455,219 AMethod of reducing coke yield198499
US 4,518,487 AProcess for improving product yields from delayed coking198584
US 4,575,413 AAluminum stearate and/or acetate antifoulants for refinery operations198627
EP 0,266,872 A1Mixed base complex antifoulant compositions and use thereof—8
EP 0,267,674 A1Antifoulant compositions and uses thereof—17
US 4,832,823 ACoking process with decant oil addition to reduce coke yield198925
US 4,927,519 AMethod for controlling fouling deposit formation in a liquid hydrocarbonaceous medium using multifunctional antifoulant compositions199068
WO 9,306,195 A1Overbased metal-containing detergents—15
US 5,407,560 AProcess for manufacturing petroleum cokes and cracked oil from heavy petroleum oil199532
US 5,567,305 AMethod for retarding corrosion and coke formation and deposition during pyrolytic hydrocarbon processing199643
US 5,853,565 AControlling thermal coking199852
US 6,197,075 B1Overbased magnesium deposit control additive for residual fuel oils200139
US 6,803,029 B2Process for reducing metal catalyzed coke formation in hydrocarbon processing200435
WO 2004/104139 A1Delayed coking process for producing free-flowing shot coke—32
WO 2005/087898 A1Method for improving liquid yield during thermal cracking of hydrocarbons—2