Patents
US 7,422,968 B2#28735743 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacturing a semiconductor device having silicided regions

3Forward Citations (#28735743 Global)
0.2/yrCitation Velocity (#36175641 Global)
1.43Citation PageRank (#24567607 Global)
20Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a method for manufacturing a semiconductor device, and a method for manufacturing an integrated circuit including the semiconductor devices. The method for manufacturing a semiconductor device ( 100 ) , among other steps, includes forming a gate structure ( 120 ) over a substrate ( 110 ) and forming source/drain regions ( 190 ) in the substrate ( 110 ) proximate the gate structure ( 120 ). The method further includes subjecting the gate structure ( 120 ) and substrate ( 110 ) to a dry etch process and placing fluorine in the source/drain regions to form fluorinated source/drains ( 320 ) subsequent to subjecting the gate structure ( 120 ) and substrate ( 110 ) to the dry etch process. Thereafter, the method includes forming metal silicide regions ( 510, 520 ) in the gate structure ( 120 ) and the fluorinated source/drains ( 320 ).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 3.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a semiconductor device, comprising: forming a gate structure over a substrate; forming source/drain regions in the substrate proximate the gate structure; after forming source/drain regions, subjecting the gate structure and substrate to a dry etch process; placing fluorine in the source/drain regions to form fluorinated source/drains subsequent to subjecting the gate structure and substrate to the dry etch process; and forming metal silicide regions in the gate structure and in the fluorinated source/drains wherein forming metal suicide regions includes forming a me

  2. Claim 2Independent Claim

    The method as recited

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 5,685,941 AInductively coupled plasma reactor with top electrode for enhancing plasma ignition199761
US 5,807,770 AFabrication method of semiconductor device containing semiconductor active film199844
US 5,866,451 AMethod of making a semiconductor device having 4t sram and mixed-mode capacitor in logic199945
US 5,885,861 AReduction of dopant diffusion by the co-implantation of impurities into the transistor gate conductor199971
US 5,895,245 APlasma ash for silicon surface preparation199920
US 5,950,098 AManufacturing method of a semiconductor device with a silicide layer199922
US 6,248,637 B1Process for manufacturing MOS Transistors having elevated source and drain regions200155
US 6,300,664 B1Semiconductor device and method of fabricating the same200133
US 2001045605 A1Semiconductor device comprising metal silicide films formed to cover gate electrode and source-drain diffusion layers and method of manufacturing the same—24
US 2002168828 A1Method of reducing threshold voltage shifting of a gate—21
US 6,534,390 B1Salicide method for producing a semiconductor device using silicon/amorphous silicon/metal structure200319
US 2003068866 A1Method for forming a self-aligned silicide of a metal oxide semiconductor—11
US 2003080352 A1Mosfet structure with reduced junction capacitance—7
US 2003092273 A1Method of manufacturing a semiconductor device employing a fluorine-based etch substantially free of hydrogen—3
US 2003203562 A1Power switching transistor and method of manufacture for a fluid ejection device—3
US 6,740,570 B2Method for forming a self-aligned silicide of a metal oxide semiconductor20048
US 2004183220 A1Ultra thin layer coating using self-assembled molecules as a separating layer for diffraction grating application—17
US 6,884,736 B2Method of forming contact plug on silicide structure200520
US 6,902,966 B2Low-temperature post-dopant activation process20057
US 6,911,384 B2Gate structure with independently tailored vertical doping profile200521