Low temperature process to produce low-K dielectrics with low stress by plasma-enhanced chemical vapor deposition (PECVD)

14Forward Citations (#6942980 Global)
0.8/yrCitation Velocity (#9561317 Global)
2.48Citation PageRank (#10271131 Global)
47Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Low K dielectric films exhibiting low mechanical stress may be formed utilizing various techniques in accordance with the present invention. In one embodiment, carbon-containing silicon oxide films are formed by plasma-assisted chemical vapor deposition at low temperatures (300° C. or less). In accordance with another embodiment, as-deposited carbon containing silicon oxide films incorporate a porogen whose subsequent liberation reduces film stress.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 14.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of depositing a carbon-doped silicon oxide film on a wafer, the method comprising: mixing a silicon containing precursor with a carbon containing precursor in the presence of a plasma to deposit a carbon doped silicon oxide film having a stress of about 20 MPa or less; wherein as deposited, the carbon-doped silicon oxide film comprises a porogen, the method further comprising: annealing the as-deposited carbon doped silicon oxide film to liberate the porogen.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the porogen comprises a linear organic molecule.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the porogen comprises a cyclic organic molecule.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (47)

PatentTitleYearCitations
US 5,003,128 AElectrical switch and outlets protecting cover for painting199184
US 5,362,526 APlasma-enhanced CVD process using TEOS for depositing silicon oxide1994252
US 5,468,595 AMethod for three-dimensional control of solubility properties of resist layers199598
WO 9,941,423 A2Plasma processes for depositing low dielectric constant films—169
US 6,042,994 ANanoporous silica dielectric films modified by electron beam exposure and having low dielectric constant and low water content200085
US 6,132,814 AMethod for curing spin-on-glass film utilizing electron beam radiation2000104
US 6,150,070 AMethod of creating optimal profile in single layer photoresist200019
US 6,177,143 B1Electron beam treatment of siloxane resins200157
US 6,195,246 B1Electrostatic chuck having replaceable dielectric cover200128
US 6,204,201 B1Method of processing films prior to chemical vapor deposition using electron beam processing200174
US 6,207,555 B1Electron beam process during dual damascene processing200169
US 6,218,090 B1Method of creating controlled discontinuity between photoresist and substrate for improving metal lift off200120
US 6,255,035 B1Method of creating optimal photoresist structures used in the manufacture of metal T-gates for high-speed semiconductor devices200180
EP 1,119,035 A2Method for depositing a low dielectric constant film—35
US 6,271,146 B1Electron beam treatment of fluorinated silicate glass200154
WO 0,161,737 A1Electron beam modification of cvd deposited films, forming low dielectric constant materials—23

Non-Patent Literature (2)

  • Demos et al., "A Thermally Stable, k<2.5 Carbon-Doped Oxide Film Deposited by a Plasma-Enhance CVD Process," Microsoft Power Point presentation, Applied Materials, Santa Clara, CA, USA, May 11, 2004, 21 pages total.
  • Dixit et al., "Film Properties and Integration Performance of a Nano-Porous Carbon Doped Oxide," Microsoft Power Point presentation, Applied Materials, Santa Clara, CA, USA, May 11, 2004, 22 pages total.