Copper alloy

3Forward Citations (#32232000 Global)
0.2/yrCitation Velocity (#36448311 Global)
1.11Citation PageRank (#36075433 Global)
12Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Raw materials for a copper alloy are melted in a high frequency smelter and cast, and milling, rolling, and annealing are carried out. Then, rolling is again carried out. Thereafter, the materials are heated at a temperature of 900° C. for one minute and are quenched in water, to be solution treated. Subsequently, the materials are heated at a temperature of 500° C. for five hours for aging, and then are cooled at a cooling rate in a range of 10 to 50° C. per hour until the materials are cooled to a temperature of 380° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A copper alloy comprising: Ni in an amount of 2.2 to 3.2 percent by mass; Si in an amount of 0.4 to 0.8 percent by mass; Cu and an unavoidable impurity, wherein a mass ratio of said Ni to said Si is in a range of 4.0 to 5.5, and a size of an inclusion precipitated in said copper alloy is equal to or smaller than 2 μm, and a total volume of said inclusion precipitated which is 0.1 to 2 μm in size is smaller than 0.5% of a total volume of said copper alloy, wherein said copper alloy has a tensile strength equal to or higher than 800 MPa.

  2. Claim 2Depends on #1

    The copper alloy according to claim 1 , further comprising Zn of 0.1 to 1.0 percent by mass.