Ultrafine mixed-crystal oxide, production process and use thereof
Abstract
An ultrafine mixed-crystal oxide, wherein the oxide has a change in absorbance of about 5 (/hr) or less when measured in such a manner that said oxide is dispersed at a concentration of 0.067% in a solvent of a 98% glycerin in which Sunset Yellow is dissolved at a concentration of 0.02%, thereby preparing a dispersion, and the dispersion is irradiated with a BLB lamp (ultraviolet light) with an intensity of 1.65 mW/cm 2 to obtain said change in absorbance (ΔOD) at 490 nm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
An ultrafine mixed-crystal oxide has a BET specific surface area of about 10 to about 200 m 2 /g, and, wherein said oxide has a change in absorbance of about 5 (/hr) or less when measured in such a manner that said oxide is dispersed at a concentration of 0.067% in a solvent of a 98% glycerin in which Sunset Yellow is dissolved at a concentration of 0.02%, thereby preparing a dispersion, and said dispersion is irradiated with a BLB lamp (ultraviolet light) with an intensity of 1.65 mW/cm 2 to obtain said change in absorbance (ΔOD) at 490 nm, and wherein said oxide comprises primary particles
- Claim 2Depends on #1
The ultrafine mixed-crystal oxide as claimed in claim 1 , w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.