Patents
US 7,368,410 B2#4681079 Most CitedExpiredUnited States (USPTO)Utility

Zeolite catalyst and method of preparing and use of zeolite catalyst

19Forward Citations (#4681079 Global)
1.1/yrCitation Velocity (#6069321 Global)
2.00Citation PageRank (#14483170 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A zeolite catalyst is prepared by treating a zeolite with a phosphorus compound to form a phosphorus-treated zeolite. The phosphorus-treated zeolite is heated to a temperature of about 300° C. or higher and combined with an inorganic oxide binder material to form a zeolite-binder mixture. The zeolite-binder mixture is heated to a temperature of about 400° C. or higher to form a bound zeolite catalyst. The bound zeolite may exhibit at least two 31 P MAS NMR peaks with maxima at from about 0 to about −55 ppm, with at least one peak having a maximum at from about −40 to about −50 ppm. Zeolites containing 10-oxygen ring pores that have been prepared in such a way may be used in aromatic alkylation by contacting the bound zeolite catalyst with an aromatic alkylation feed of an aromatic compound and an alkylating agent under reaction conditions suitable for aromatic alkylation.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a zeolite catalyst comprising: treating a zeolite with a phosphorus compound to form a phosphorus-treated zeolite; heating the phosphorus-treated zeolite to a temperature of about 300° C. or higher; combining the phosphorus-treated zeolite with an inorganic oxide binder material to form a zeolite-binder mixture; and heating the zeolite-binder mixture at temperature of about 400° C. or higher to form a bound zeolite catalyst.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein: the binder material includes at least one of alumina, clay, aluminum phosphate and silica-alumina.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein: the binder material is an alumina-containing material.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 19 total)

PatentTitleYearCitations
WO 2014/189871 A1Method for conversion of aromatic hydrocarbons—0
WO 2013/059172 A1Process for producing phosphorus modified zeolite catalysts—0
US 8,969,643 B2Method for conversion of aromatic hydrocarbons20150
DE 112012001227 T5Verbessertes Verfahren zur Herstellung eines Katalysators auf Zeolithbasis zur Umwandlung von Methanol in Olefine—0
WO 2014/025371 A1Method of making a catalyst and catalyst made thereby and its use in aromatic alkylation—2
DE 102011013911 A1Verbessertes Verfahren zur Herstellung eines Katalysators auf Zeolithbasis zur Umwandlung von Methanol in Olefine—0
WO 2012/123558 A1Process for manufacture of a zeolite based catalyst for the conversion of methanol to olefins—7
WO 2013/059176 A1Process for producing phosphorus modified zeolite catalysts—0
US 10,112,188 B2Process for manufacture of a zeolite based catalyst for the conversion of methanol to olefins20181
US 9,783,462 B2Toluene methylation with transalkylation of heavy aromatics20174
US 2014058180 A1Modified catalyst for converting oxygenates to olefins—8
US 9,821,299 B2Process for producing phosphorus modified zeolite catalysts20170
DE 102011013909 A1Verfahren zur Herstellung eines Katalysators auf Zeolithbasis zur Umwandlung von Methanol in Olefine—2
WO 2012/123556 A1Improved process for manufacture of a zeolite based catalyst for the conversion of methanol to olefins—10
US 10,005,073 B2Process for manufacture of a zeolite based catalyst for the conversion of methanol to olefins20181