Method and apparatus for flip chip attachment by post collapse re-melt and re-solidification of bumps
Abstract
A solder bump reflow process includes raising the temperature of an aligned die-substrate assembly to a temperature and for a time sufficient to cause a first reflow; allowing the temperature of the assembly to fall to a first cooling temperature and for a time sufficient to re-solidify the solder; raising the temperature of the die-substrate assembly a second time to a temperature and for a time sufficient to cause a second reflow; allowing the temperature of the assembly to fall a second time to a second cooling temperature and eventually to an ambient room temperature; in which at least the first and second melts and the first re-solidification are conducted without exposing the assembly to oxidizing atmosphere. Also, apparatus for carrying out the method includes a multi-zone oven.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A solder bump reflow process, comprising: providing a die having a plurality of solder bumps and a substrate having a plurality of mating surfaces on interconnect sites, the solder bumps being made with a material having a liquidus temperature and a solidus temperature; contacting the solder bumps of the die and the mating surfaces of the substrate to form a die-substrate assembly; placing the die-substrate assembly on a transport mechanism which passes through an oven having a non-oxidizing atmosphere, the oven operating with a plurality of physically separate temperature zones; passing the d
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗