Fluorinated resin water dispersion composition and fluorinated water base coating composition
Abstract
This invention provides the invention provides a fluororesin aqueous dispersion composition comprising a tetrafluoroethylene-based polymer and an aliphatic polyoxyalkylene ether dispersant incorporated therein, wherein the aliphatic polyoxyalkylene ether dispersant shows a 50% decomposition temperature of not lower than 250° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 7.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A fluororesin aqueous dispersion composition comprising a tetrafluoroethylene-based polymer and an aliphatic polyoxyalkylene ether dispersant incorporated therein, wherein said aliphatic polyoxyalkylene ether dispersant shows a 50% decomposition temperature of not lower than 250° C. and is represented by the following general formula: RO(C 2 H 4 O) n (C 3 H 6 O) m H wherein R is an alkyl group represented by —C 13 H 27 with an average number of branches of 1.5 to 2.9 per molecule, n represents an integer of 3 to 25 and m represents an integer of 0 to 6.
- Claim 2Depends on #1
The fluororesin aqueous dispersion composition according to claim 1 , wherein the aliphatic polyoxyalkylene ether dispersant shows an oxidative degradation percentage of not higher than 2% at 200° C.
- Claim 3Independent Claim
The fluororesin aqueous dispersion c
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (20)
Non-Patent Literature (4)
- "Modern Fluoropolymer", Scheir, p. 10.
- "Modern Fluoropolymers" Edited by John Scheirs, p. 240, 1997.
- "Modern Fluoropolymers", Scheirs, p. 240.
- International Search Report for PCT/JP03/06177 dated Oct. 7, 2003.