A method of manufacturing an oxide dispersion strengthened ferritic steel excellent in high-temperature creep strength having a coarse grain structure. The method comprises mixing alloy powders and an Y 2 O 3 powder, subjecting the mixed powder to mechanical alloying treatment, solidifying the alloyed powder by hot extrusion, and subjecting the extruded solidified material to final heat treatment involving heating to and holding at a temperature of not less than the Ac 3 transformation point and slow cooling at a rate of not more than a ferrite-forming critical rate which comprises, 0.05-0.25% C, 8.0-12.0% Cr, 0.1-4.0% W, 0.1-1.0% Ti, 0.1-0.5% Y 2 O 3 by weight, with the balance being Fe. In this method, by using a TiO 2 powder as a Ti component to be mixed at the mechanical alloying treatment or by adding a Fe 2 O 3 powder, the bonding of Ti with C is suppressed, and the C concentration in the matrix does not decrease.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing an oxide dispersion strengthened ferritic steel excellent in high-temperature creep strength having a coarse grain structure, said method comprising mixing either element powders or alloy powders and a Y 2 O 3 powder, subjecting the mixed powder to mechanical alloying treatment, subjecting the resulting alloyed powder to hot extrusion, and subjecting the resulting extruded material to final heat treatment involving heating to and holding at a temperature of not less than the Ac 3 transformation point and slow cooling at a rate of not more than 100° C./hr to thereby

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Asabe et al. The Development of a Metal Matrix Composite by Mechanical Alloying, The Sumimoto Search, No. 45, pp. 65-72 (Mar. 1991).
  • English abstract of JP 5051709.
  • English abstract of JP 56044716.
  • English abstract of JP 63210299.
  • English abstracts of FR 2777020.