Abstract

The present invention provides methods of fabricating a radiation-absorbing semiconductor wafer by irradiating at least one surface location of a silicon substrate, e.g., an n-doped crystalline silicon, by a plurality of temporally short laser pulses, e.g., femtosecond pulses, while exposing that location to a substance, e.g., SF 6 , having an electron-donating constituent so as to generate a substantially disordered surface layer (i.e., a microstructured layer) that incorporates a concentration of that electron-donating constituent, e.g., sulfur. The substrate is also annealed at an elevated temperature and for a duration selected to enhance the charge carrier density in the surface layer. For example, the substrate can be annealed at a temperature in a range of about 700 K to about 900 K.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 70.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a radiation-absorbing semiconductor structure, comprising: irradiating each of a plurality of locations on a surface of a silicon substrate with one or more femtosecond laser pulses while exposing said surface to a sulfur-containing substance so as to generate a plurality of sulfur inclusions in a surface layer of said substrate, and annealing said substrate at a temperature in a range of about 500 K to about 1100 K for a time duration in a range of about a few seconds to about a few hours.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising selecting a duration of each laser pulse to be in a range of about 50 femtoseconds to about 500 femtoseconds.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising selecting a fluence of each pulse to be in a range of about 1 kJ/m 2 to about 15 kJ/m 2 .

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Carey et al., "Fabrication Of Micrometer-Sized Conical Field Emitters Using Femtosecond Laser-Assisted Etching Of Silicon", International Vacuum Microelectronics Conference 2001 (Davis, CA, 2001) 75-76.
  • Carey et al., "Femtosecond Laser-Assisted Microstructuring Of Silicon For Novel Detector, Sensing And Display Technologies", LEOS 2002 (Glasgow, Scotland, 2002) 97-98.
  • Carey et al., "Femtosecond Laser-Assisted Microstructuring Of Silicon For Novel Detector, Sensing And Display Technologies", LEOS Oct. 26, 2003 (Tuscon, AR, 2003) 481-482.
  • Carey et al., "Femtosecond-Laser-Assisted Microstructuring Of Silicon Surfaces", Optics and Photonics News, 14, 32-36 (2003).
  • Carey et al., "Field Emission From Silicon Microstructures Formed By Femtosecond Laser Assisted Etching", CLEO 2001 (Baltimore, MD, 2001) 555-556.