Metalothermic reduction of refractory metal oxides

11Forward Citations (#9400152 Global)
0.6/yrCitation Velocity (#12938841 Global)
2.12Citation PageRank (#13196505 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of producing a refractory metal powder by (A) combining (i) an oxide particle component and (ii) a reducing agent; (B) forming a substantially uniform mixture of (i) and (ii); (C) continuously feeding the mixture into a furnace; (D) igniting the mixture at a reaction zone and starting a reaction that is sufficiently exothermic to form a high temperature flash; (E) starting a reaction that is sufficiently exothermic to form a high temperature self-sustaining flash; and (F) producing a free-flowing reduced oxide powder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a refractory metal powder comprising: (A) blending (i) an oxide particle component which contains a refractory metal and said refractory metal is tantalum or niobium and (ii) a solid reducing agent; (B) forming a substantially uniform mixture of (i) and (ii); (C) continuously feeding the mixture into a furnace; (D) igniting the mixture at a reaction zone and staffing a reaction that is form a high temperature exothermic to form a high temperature flash; (E) starting a reaction that is sufficiently exothermic to form a high temperature self-sustaining flash; and (F) produc