Method for forming via hole and trench for dual damascene interconnection
Abstract
A method for forming a via hole and a trench for a dual damascene interconnection comprises forming a via hole through an inter-metal insulating film to expose a portion of a surface of an etch stop film on a lower metal film, forming a photoresist film on an entire surface of the resultant structure and in the via hole, exposing a top surface and a side surface of the inter-metal insulating film by recessing the photoresist film using a development process for the photoresist film, forming a bottom antireflective coating film on the exposed surfaces of the inter-metal insulating film and the photoresist film, forming a mask pattern on the bottom antireflective coating film, forming a trench by an etching process using the mask pattern as an etch mask, and completely removing the photoresist film within the via hole.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for forming a via hole and a trench for a dual damascene interconnection, comprising: forming a via hole through an inter-metal insulating film to expose a portion of a surface of an etch stop film on a lower metal film; forming a photoresist film on an entire surface of the resultant structure and in the via hole; exposing a top surface and a side surface of the inter-metal insulating film by recessing the photoresist film using a development process for the photoresist film; forming a bottom antireflective coating film on the exposed surfaces of the inter-metal insulating film and t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2009170221 A1 | Etch residue reduction by ash methodology | — | 3 |
| US 7,910,477 B2 | Etch residue reduction by ash methodology | 2011 | 2 |