Patents
US 7,329,610 B2#30219350 Most CitedExpiredUnited States (USPTO)Utility

Method of high selectivity SAC etching

3Forward Citations (#30219350 Global)
0.2/yrCitation Velocity (#36317202 Global)
1.23Citation PageRank (#30724394 Global)
21Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for SAC etching is provided involving a) etching a Si wafer having a nitride present thereon with a first etching gas containing a first perfluorocarbon and carbon monoxide, and b) etching the resultant Si wafer having an initially etched nitride photoresist thereon with a second etching gas containing a second perfluorocarbon in the substantial absence of carbon monoxide, wherein the etching steps a) and b) are performed at high RF power and low pressure compared to conventional processes to provide higher selectivity etching and a larger process window for SAC etching, as well as the ability to perform SAC etching and island contact etching under the same conditions with high verticality of the island contact and SAC walls.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for etching of silicon oxide/silicon nitride structure, comprising: (a) etching a silicon oxide layer above a silicon nitride layer present thereon with a first etching gas comprising a first perfluorocarbon and carbon monoxide to a point where a part of the silicon nitride layer is exposed and a portion of the silicon oxide layer is left unetched, and b) etching the unetched portion of the silicon oxide layer above the silicon nitride layer with a second etching gas comprising a second perfluorocarbon in the absence of carbon monoxide to etch through the silicon oxide layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said step a) and step b) are each performed at a plasma producing RF power of greater than 1500 W and at a pressure of 50 mTorr or less.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein said step a) is performed at a plasma producing RF power of at

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
EP 0,726,596 A2Plasma etching method—15
US 5,595,627 APlasma etching method1997143
US 5,811,357 AProcess of etching an oxide layer199856
WO 9,934,419 A1Etching process—14
JP H11186229 ADry etching and manufacture of semiconductor device—20
DE 19,929,239 A1MOSFET integrated circuit manufacture lithography masking technique—3
JP 2000036491 AFabrication of semiconductor device—13
US 6,033,962 AMethod of fabricating sidewall spacers for a self-aligned contact hole200040
US 6,066,555 AMethod for eliminating lateral spacer erosion on enclosed contact topographies during RF sputter cleaning200030
US 6,121,098 ASemiconductor manufacturing method200038
US 6,143,615 AMethod of forming a resistor20004
US 6,159,862 ASemiconductor processing method and system using C5 F8200077
US 6,168,989 B1Process for making new and improved crown-shaped capacitors on dynamic random access memory cells200132
US 6,211,092 B1Counterbore dielectric plasma etch process particularly useful for dual damascene2001127
US 6,221,772 B1Method of cleaning the polymer from within holes on a semiconductor wafer200130
US 2002030174 A1Etchant for use in a semiconductor processing method and system—8
US 6,399,511 B2Plasma etch process in a single inter-level dielectric etch200247
US 6,451,703 B1Magnetically enhanced plasma etch process using a heavy fluorocarbon etching gas200258
US 6,465,359 B2Etchant for use in a semiconductor processing method and system200222
US 6,602,435 B1Etching method20033
US 6,803,318 B1Method of forming self aligned contacts200493