Abstract
A refractory container for evaporating metals, having significantly improved useful life and corrosion resistance properties, said container consists essentially of a refractory boride, boron nitride, and about 0.10 to 10 wt. % of a rare earth metal compound selected from one of an oxide, a nitride, a carbide, or mixtures thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A refractory container for evaporating metals, said refractory container consisting essentially of: a) about 45 to 65 wt. % of boron nitride; b) about 35 to 65 wt. % of a refractory boride; and c) about 0.10 to 10 wt. % of a rare earth metal compound selected from YAG (Al 5 Y 3 O 12 ), YAP (AlYO 3 ), YAM (Al 2 Y 4 O 7 ), and combinations thereof.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (3)
- Esk Engineered Ceramincs-Wacker Chemicals article, "The Effects of Boat and Wire Parameters on Boat Life and Coating Quality in Vacuum Metallization of an OPP Web", E.Josephson, et al.
- Machine translation of Japanese document 06-298566, Oct. 25, 1994.
- XP002327970, May 27, 1988, Japan abstract.