Patents
US 7,316,745 B2#5745678 Most CitedExpiredUnited States (USPTO)Utility

High-resistance silicon wafer and process for producing the same

16Forward Citations (#5745678 Global)
0.9/yrCitation Velocity (#8030378 Global)
3.03Citation PageRank (#7438724 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A high-resistance silicon wafer is manufactured, in which a gettering ability and economical efficiency is excellent and an oxygen thermal donor is effectively prevented from being generated in a heat treatment for forming a circuit, which is to be implemented on the side of a device manufacturer. In order to implement the above, a high-temperature heat treatment at 1100° C. or higher is performed on a carbon doped high-resistance and high-oxygen silicon wafer in which specific resistivity is 100 Ωcm or more and a carbon concentration is 5×10 15 to 5×10 17 atoms/cm 3 so that a remaining oxygen concentration becomes 6.5×10 17 atoms/cm 3 or more (Old-ASTM). As this high-temperature treatment, an OD treatment for forming a DZ layer on a wafer surface, a high-temperature annealing treatment for eliminating a COP on the surface layer, a high-temperature heat treatment for forming a BOX layer in a SIMOX wafer manufacturing process and the like can be used.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A high-resistance silicon wafer having resistivity of 100 Ωcm or more, wherein a carbon concentration is 5×10 15 atoms/cm 3 , and wherein an oxygen concentration is over 8×10 17 atoms/cm 3 (Old-ASTM).

  2. Claim 2Depends on #1

    The high-resistance silicon wafer according to claim 1 , wherein a DZ (Denuded Zone) layer is formed at least 5 μm or more in depth from a surface of the wafer.

  3. Claim 3Depends on #1

    The high-resistance silicon wafer according to claim 1 , wherein a density of a LPD (Light Point Defect) having a size of 0.12 or more and observed on a surface of the wafter is controlled so as to be 02/cm 2 or less.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Babich, V.M. et al., 'Generation of thermal donors as a result of one- and two-step annealing of silicon crystals with large and small carbon concentrations', Semiconductors, vol. 30, No. 5, pp. 417 to 419, May 1996.
  • Gaworzewski P. et al., 'Oxygen-Related Donors Formed at 600° C in Silicon in Dependence on Oxygen and Carbon Content', Phys.Stat.Sol. (a), vol. 77, No. 2, pp. 571 to 582, 1983.
  • Kodate, Junichi et al., Suppression of Substrate Crosstalk in Mixed-Signal Complementary MOS Circuits Using High-Resistivity SIMOX (Separation by IMplanted OXygen) Wafers, Japanese Journal of Applied Physics, Part 1, vol. 39, No. 4B, pp. 2256 to 2260, Apr. 2000.
  • Wijaranakula, W. et al., 'A Formation of Crystal Defects in Carbon-Doped Czochralski-Grown Silicon after a Three-Step Internal Gettering Anneal', Journal of Electrochemical Society, vol. 138, No. 7, pp. 2153 to 2159, Jul. 1991.