Aluminum-free borosilicate glass and applications thereof
Abstract
The fluorescent lamp is made with an aluminum-free borosilicate glass having a composition, in percent by weight, based on oxide content of: SiO 2 , 65-77; B 2 O 3 , 7-20; Li 2 O, 0-2; Na 2 O, 0-4; K 2 O, 3-12; MgO, 0-2; CaO, 0-2; with MgO+CaO, 0-3; BaO, 0-3; ZnO, 0-2; ZrO 2 , 0.8-12; TiO 2 , 0-10; CeO 2 , 0-1; and F − , 0-0.6. Preferred embodiments with more than 1% by weight TiO 2 have especially good UV blocking properties and are especially suitable for lamp glass for backlights. Other embodiments have good sealing properties to tungsten, KOVAR®, and molybdenum and have coefficients of thermal expansion α of 4.7 to 5.3×10 −6 /K, good chemical resistance, and a working point V A of between 990° C. and 1290° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A fluorescent lamp comprising a lamp glass, said lamp glass consisting of an aluminum-free borosilicate glass, said aluminum-free borosilicate glass having chemical resistance and a composition, in percent by weight, based on oxide content, of: SiO 2 60-78 B 2 O 3 7-20 Li 2 O 0-2 Na 2 O 0-4 K 2 O 3-12
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗