Patents
US 7,309,742 B2#22462666 Most CitedExpiredUnited States (USPTO)Utility

Impact copolymer with optimized melt flow, stiffness, and low-temperature impact resistance

5Forward Citations (#22462666 Global)
0.3/yrCitation Velocity (#28126973 Global)
1.10Citation PageRank (#36778907 Global)
3Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An impact copolymer having a flexural modulus (ASTM D-790) of at least about 1,100 MPa; a melt flow rate (ASTM D-1238) of at least about 15 g/10 min; and a maximum load under Dynatup Impact test (ASTM D-3763) of equal to or greater than about 1,700 N at a temperature of less than or equal to about −40° C. and articles of manufacture from same.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An ethylene-propylene impact copolymer having the following physical properties: a flexural modulus (ASTM D-790) of at least 1,100 MPa; a melt flow rate (ASTM D-1238) of at least 25 g/10 mm; and a maximum load under Dynatup Impact test (ASTM D-3763) of equal to or greater than 1,700 N at a temperature of greater than or equal to about −40° C.

  2. Claim 2Depends on #1

    The impact copolymer of claim 1 wherein the Dynatup Impact test is performed at a velocity of 6 m/s.

  3. Claim 3Depends on #1

    The impact copolymer of claim 1 wherein the Dynatup Impact test is performed at a velocity of 8.5 m/s.

Technical Overview & Description