Method for forming dual etch stop liner and protective layer in a semiconductor device

9Forward Citations (#11697636 Global)
0.5/yrCitation Velocity (#17554461 Global)
2.03Citation PageRank (#14179419 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a semiconductor device having dual nitride liners, a silicide layer, and a protective layer beneath one of the nitride liners for preventing the etching of the silicide layer. A first aspect of the invention provides a method for use in the manufacture of a semiconductor device comprising the steps of applying a protective layer to a device, applying a first silicon nitride liner to the device, removing a portion of the first silicon nitride liner, removing a portion of the protective layer, and applying a second silicon nitride liner to the device.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for use in the manufacture of a semiconductor device comprising the steps of: applying a protective layer to a silicide layer of a device; applying a first silicon nitride liner to the protective layer; removing a portion of the first silicon nitride liner; removing a portion of the protective layer; and applying a second silicon nitride liner directly to the silicide layer of the device.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising the step of removing a portion of the second silicon nitride liner.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the first silicon nitride liner is formed by at least one of PECVD, RTCVD, and LPCVD.