Method of manufacturing a semiconductor device
Abstract
It is intended to achieve the reduction in number of heat treatments carried out at high temperature (at least 600 ° C.) and the employment of lower temperature processes ( 600 ° C. or lower), and to achieve step simplification and throughput improvement. In the present invention, a barrier layer ( 105 ), a second semiconductor film ( 106 ), and a third semiconductor layer ( 108 ) containing an impurity element (phosphorus) that imparts one conductive type are formed on a first semiconductor film ( 104 ) having a crystalline structure. Gettering is carried out in which the metal element contained in the first semiconductor film ( 104 ) is allowed to pass through the barrier layer ( 105 ) and the second semiconductor film ( 106 ) by a heat treatment to move into the third semiconductor film ( 107 ). Afterward, the second and third semiconductor films ( 106 ) and ( 107 ) are removed with the barrier layer ( 105 ) used as an etching stopper.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a semiconductor device comprising the steps of: adding a metal element to a first semiconductor film comprising amorphous silicon over a substrate; crystallizing the first semiconductor film to form a first crystalline semiconductor film containing oxygen at a first concentration; forming a second semiconductor film containing oxygen at a second concentration over the first crystalline semiconductor film; forming a third semiconductor film containing one conductive type impurity element over the second semiconductor film; reducing a concentration of the metal element
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗