Patents
US 7,306,026 B2#1469570 Most CitedExpiredUnited States (USPTO)Utility

Cooled turbine airfoils and methods of manufacture

39Forward Citations (#1469570 Global)
2.0/yrCitation Velocity (#1927385 Global)
4.95Citation PageRank (#3365591 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An investment casting pattern is formed by installing a first core to a first element of a molding die to leave a first portion of the first core protruding from the first element. After the installing, the first element is assembled with a feed core and a second element of the molding die so that the first portion contacts the feed core. A material is molded at least partially over the first core and the feed core. The first portion has one or more surface area enhancements.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 39.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: forming an investment casting core precursor having a spine and a plurality of tine precursors; and after forming the tine precursors, forming a plurality of surface enhancement recesses in the tine precursors.

  2. Claim 2Depends on #1

    The method of claim 1 further comprising: deforming the tine precursors to at least partially spiral.

  3. Claim 3Depends on #1

    The method of claim 1 wherein: the forming the investment casting core precursor comprises at least one of: stamping; laser cutting; water jet cutting; electro-chemical machining; and electrical discharge machining.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗