Method for producing a scintillator ceramic
Abstract
A method for producing high-density, translucent, scintillator ceramics by way of a pressure-less sintering carried out at an elevated temperature. According to the method, particles of a MOS composition are prepared using a specific wet milling method whereby being reduced, in particular, to a particle size of less than 10 μm. The particles are compacted to form compacted bodies with green densities of up to 50% and higher. The sintering may be carried out under specific sintering parameters.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
Method for producing a high-density, translucent scintillator ceramic, the method comprising: doping a metal oxysulfide (MOS) with specific rare earth elements (Ln), wherein the metal oxysulfide (MOS) has the generic formula (I) (M 1-x Ln x ) 2 O 2 S Formula (I) wet milling a powder of the doped metal oxysulfide with the addition of an organic milling fluid until a particle size of the powder is <10 μm, wherein the powder has a specific surface area of 10 m 2 /g; producing a powder body from the powder, wherein the powder body has a green density selected from the range 40% to 60% inclusiv
- Claim 2Depends on #1
The method according to claim 1 , wherein the generic formula (I) M is at least one element select
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗