Patents
US 7,303,627 B2#60664305 Most CitedExpiredUnited States (USPTO)Utility

Method for making low-stress large-volume not-(111)-oriented crystals with reduced stress birefringence and more uniform refractive index and crystals made thereby

1Forward Citations (#60664305 Global)
0.1/yrCitation Velocity (#54847008 Global)
0.76Citation PageRank (#60664305 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method is described for making an especially not-(111)-oriented low-stress large-volume crystal having a glide plane with reduced stress birefringence and more uniform refractive index. The method includes growing and tempering the crystal while heating and/or cooling to form a temperature gradient in order to relax stresses arising along the glide plane. During the tempering the heating and/or cooling occurs by heat transfer in a heat transfer direction and the heat transfer direction or temperature gradient is oriented at an angle of from 5° to 90° to the glide plane. Crystals with a uniform refractive index with variations of less than 0.025×10 −6 (RMS value) are produced by the method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of making a low-stress large-volume crystal that has an orientation that is not a (111)-orientation, having a glide plane with a reduced stress birefringence and more uniform refractive index, said method comprising growing and tempering the crystal while heating and/or cooling while forming a temperature gradient in order to relax stresses arising along the glide plane; wherein during the tempering said heating and/or said cooling occurs by heat transfer in a heat transfer direction, and wherein said heat transfer direction or the temperature gradient is oriented at an angle of great

  2. Claim 2Depends on #1

    The method as defined in claim 1 , wherein the angle between the glide plane and the temperature gradient is between 25° to 65°.

  3. Claim 3Depends on #1

    The method as defined in claim 1 , wherein the angle between the glide plane and the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
EP 0,213,514 B1Aqueous liquid preparation19900
JP H10251096 AMethod for annealing fluorite single crystal—9
EP 0,939,147 A2A manufacturing method for calcium fluoride and calcium fluoride for photolithography—40
EP 0,942,297 A2Optical element made from fluoride single crystal and method of manufacturing the optical element—30
EP 0,972,863 A1Method for annealing single crystal fluoride and method for manufacturing the same—28
DE 10,010,484 A1Device for growing large volume single crystals has heating element arranged on side walls of melt crucible to prevent lateral radial heat flow—10
DE 10,010,485 A1Verfahren zur Herstellung von hochhomogenen, grossformatigen Einkristallen aus Calciumfluorid sowie deren Verwendung—5
JP 2001335398 ALarge diameter fluorite single crystal for photolithography and its production method—10
US 6,332,922 B1Manufacturing method for calcium fluoride and calcium fluoride for photolithography200137
US 2003089306 A1Method for producing crystal and/or crystal materials containing fluorine—13
US 2003089307 A1Method and device for growing large-volume oriented monocrystals—33
JP 2003327499 AMethod of producing single crystal—9
US 2004005266 A1Optical member, process for producing the same, and projection aligner—12
US 2004016743 A1Substantially-uniform-temperature annealing—31
US 2004099205 A1Method of growing oriented calcium fluoride single crystals—26
US 2004251851 A1Flashing discharge tube-use power supply and control method therefor—14

Non-Patent Literature (1)

  • John H. Burnett et al: "Intrinsic Birefringence in Calcium Fluoride . . . ", Physical Review B, vol. 64, 2001, 241102-1-241102-4.