Patents
US 7,300,958 B2#2400754 Most CitedExpiredUnited States (USPTO)Utility

Ultra-dispersed nanocarbon and method for preparing the same

29Forward Citations (#2400754 Global)
1.5/yrCitation Velocity (#3358167 Global)
4.40Citation PageRank (#4087018 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Ultradispersed ones of primary particles of nanometer-sized carbon are obtained by applying a wet-type milling method and/or a wet dispersion method to an aggregate structure of the primary particles to overcome van der Waals forces, by which forces the primary particles are held together to form the aggregate structure, whereby the ultradispersed primary particles are obtained in a colloidal dispersion on a large-scale basis at low cost without using any additive. In a method of manufacturing the ultradispersed primary particles, the wet-type milling method is carried out in a ball mill, preferably in combination with a high-energy ultrasonic-wave process carried out in a dispersing medium such as pure water, whereby a colloidal solution or slurry with a low-concentration of the primary particles ultradispersed in the dispersing medium is obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 29.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing an ultradispersion of primary particles of nanometer-sized carbon, comprising: applying a wet milling method to an aggregate structure of said primary particles of nanometer-sized carbon to overcome van der Waals forces, by which forces said primary particles of nanometer-sized carbon are held together to form said aggregate structure, wherein said wet milling method is carried out with balls as a breaking medium, each of the balls having a diameter less than or equal to 0.1 mm.

  2. Claim 2Depends on #1

    The method of manufacturing as set forth in claim 1 , wherein said structure is subjected to said wet milling method in water or in an organic solvent.

  3. Claim 3Depends on #1

    The method of manufacturing as set forth in claim 1 , wherein, after completion of said wet milling method, said primary particles of nanometer-sized carbon are subjected to an ultraso

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Perry, Robert H. et al., Size Reduction and Size Enlargement, Perry's Handbook, Seventh Edition, 1997, Table 20-18, p. 20-38.