Patents
US 7,291,920 B2#22454789 Most CitedExpiredUnited States (USPTO)Utility

Semiconductor structures

5Forward Citations (#22454789 Global)
0.3/yrCitation Velocity (#28126702 Global)
1.10Citation PageRank (#36509033 Global)
36Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In one aspect, the invention includes a method of forming a roughened layer of platinum, comprising: a) providing a substrate within a reaction chamber; b) flowing an oxidizing gas into the reaction chamber; c) flowing a platinum precursor into the reaction chamber and depositing platinum from the platinum precursor over the substrate in the presence of the oxidizing gas; and d) maintaining a temperature within the reaction chamber at from about 0° C. to less than 300° C. during the depositing. In another aspect, the invention includes a platinum-containing material, comprising: a) a substrate; and b) a roughened platinum layer over the substrate, the roughened platinum layer having a continuous surface characterized by columnar pedestals having heights greater than or equal to about one-third of a total thickness of the platinum layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A semiconductor structure, comprising: a semiconductive substrate; a roughened platinum layer over the substrate, the roughened platinum layer having a continuous surface characterized by columnar pedestals having heights greater than or equal to about one-third of a total thickness of the platinum layer; and an adhesion layer between the roughened platinum layer and the substrate, and against both the roughened platinum layer and the substrate, the adhesion layer comprising one or more of iridium, rhodium, ruthenium, platinum, palladium, osmium, and silver.

  2. Claim 2Depends on #1

    The structure of claim 1 wherein the roughened platinum layer has a thickness of at least about 600 Å.

  3. Claim 3Depends on #1

    The structure of claim 1 wherein the roughened platinum layer has a thickness of greater than or equal to about 400 Å.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
US 3,856,709 ACoating a substrate with soft particles197424
US 3,975,304 ACoating a substrate with soft particles197627
US 4,341,662 AMethod of catalytically coating low porosity ceramic surfaces198223
US 4,425,261 ALiquid suspension of particles of a metal belonging to the platinum group and a method for the manufacture of such a suspension198488
US 4,431,750 APlatinum group metal catalyst on the surface of a support and a process for preparing same198472
US 4,714,693 AMethod of making a catalyst composition comprising uniform size metal components on carrier198777
US 4,719,442 APlatinum resistance thermometer198821
EP 0,415,751 A1Thin film capacitor and manufacturing method thereof—46
US 5,053,917 AThin film capacitor and manufacturing method thereof1991171
JP H0567730 AStructure of semiconductor element and manufacture thereof—17
US 5,208,479 AMethod of increasing capacitance of polycrystalline silicon devices by surface roughening and polycrystalline silicon devices199343
US 5,320,978 ASelective area platinum film deposition199438
US 5,330,700 APorous electrode for a pacemaker and method of making same199418
JP H0817939 ASemiconductor device and manufacture thereof—10
US 5,525,570 AProcess for producing a catalyst layer on a carrier and a catalyst produced therefrom199658
US 5,555,486 AHybrid metal/metal oxide electrodes for ferroelectric capacitors1996204
JP H0951079 ASemiconductor element and manufacture thereof—10
JP H0982666 AFormation of thin film, semiconductor device and manufacture thereof—15
US 5,635,420 AMethod of making a semiconductor device having a capacitive layer199735
US 5,639,685 ASemiconductor processing method of providing a conductively doped layer of hemispherical grain polysilicon199769
JP H09239891 ADielectric thin film and method for forming the film—8
US 5,763,286 AProcess for manufacturing a DRAM capacitor having an annularly-grooved, cup-shaped storage-node plate which stores charge on inner and outer surfaces199881
JP H10173149 ASemiconductor device and its manufacture—10
JP H10180098 AProduction of catalyst for purification of exhaust gas and apparatus therefor—8
US 5,783,716 APlatinum source compositions for chemical vapor deposition of platinum199854

Non-Patent Literature (3)

  • Characterization of Pt Thin Films Deposited . . . , 1997, Kwon, et al.
  • Rugged Surface Poly-crystalline Silicon . . . , 1996, Ino, et al.