US 7,288,808 B2#103432767 Most CitedExpiredUnited States (USPTO)Utility

Capacitor constructions with enhanced surface area

0Forward Citations (#103432767 Global)
0.0/yrCitation Velocity (#103432767 Global)
0.56Citation PageRank (#103432767 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A capacitor fabrication method may include forming a first capacitor electrode over a substrate, the first electrode having an inner surface area per unit area and an outer surface area per unit area that are both greater than an outer surface area per unit area of the substrate. A capacitor dielectric layer and a second capacitor electrode may be formed over the dielectric layer. The method may further include forming rugged polysilicon over the substrate, the first electrode being over the rugged polysilicon. Accordingly, the outer surface area of the first electrode can be at least 30% greater than the outer surface area of the substrate without the first electrode including polysilicon.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A capacitor construction comprising: an opening in an insulative layer over a substrate, the opening having sides and a bottom; a hemispherical grain polysilicon layer over the sides of the opening but not over the bottom; a conformal first capacitor electrode containing TiN on the polysilicon, the first electrode being sufficiently thin that the first electrode has a rugged outer surface with an outer surface area per unit area greater than an outer surface area per unit area of the substrate underlying the first electrode; a capacitor dielectric layer on the first electrode; and a second cap

  2. Claim 2Depends on #1

    The construction of claim 1 wherein the polysilicon is undoped.

  3. Claim 3Depends on #1

    The construction of claim 1 wherein the polysilicon comprises spaced apart grains.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,006,956 ADielectric ceramic composition199119
US 5,126,283 AProcess for the selective encapsulation of an electrically conductive structure in a semiconductor device199254
US 5,187,637 AMonolithic high-voltage capacitor199349
US 5,316,982 ASemiconductor device and method for preparing the same199482
US 5,432,732 ADynamic semiconductor memory199534
US 5,444,013 AMethod of forming a capacitor1995169
US 5,452,178 AStructure and method of making a capacitor for an intergrated circuit1995177
US 5,625,233 AThin film multi-layer oxygen diffusion barrier consisting of refractory metal, refractory metal aluminide, and aluminum oxide199793
US 5,641,984 AHermetically sealed radiation imager199758
US 5,811,344 AMethod of forming a capacitor of a dram cell199837
US 5,885,882 AMethod for making polysilicon electrode with increased surface area making same199929
US 5,899,725 AMethod of forming a hemispherical grained silicon on refractory metal nitride199922
US 5,905,280 ACapacitor structures, DRAM cell structures, methods of forming capacitors, methods of forming DRAM cells, and integrated circuits incorporating capacitor structures and DRAM cell structures199938
US 5,972,769 ASelf-aligned multiple crown storage capacitor and method of formation199932
US 6,033,967 AMethod for increasing capacitance in DRAM capacitors and devices formed200033
US 6,069,053 AFormation of conductive rugged silicon200041
US 6,104,049 AFerroelectric memory with ferroelectric thin film having thickness of 90 nanometers or less, and method of making same200044
US 6,124,158 AMethod of reducing carbon contamination of a thin dielectric film by using gaseous organic precursors, inert gas, and ozone to react with carbon contaminants2000197
US 6,144,060 AIntegrated circuit devices having buffer layers therein which contain metal oxide stabilized by heat treatment under low temperature2000270
US 6,156,606 AMethod of forming a trench capacitor using a rutile dielectric material200060
US 6,174,770 B1Method for forming a crown capacitor having HSG for DRAM memory200135
US 6,180,481 B1Barrier layer fabrication methods200140
US 6,180,447 B1Methods for fabricating integrated circuit capacitors including barrier layers having grain boundary filling material200140
US 6,204,070 B1Method for manufacturing ferroelectric capacitor200142
US 6,204,172 B1Low temperature deposition of barrier layers200180
US 6,207,487 B1Method for forming dielectric film of capacitor having different thicknesses partly2001300
US 6,207,561 B1Selective oxidation methods for metal oxide deposition on metals in capacitor fabrication200154
US 6,218,256 B1Electrode and capacitor structure for a semiconductor device and associated methods of manufacture200146
US 6,218,260 B1Methods of forming integrated circuit capacitors having improved electrode and dielectric layer characteristics and capacitors formed thereby200165
US 6,222,722 B1Storage capacitor having undulated lower electrode for a semiconductor device2001104

Non-Patent Literature (5)

  • A. W. Ott, et al., "Atomic Layer Controlled Deposition of Al<SUB>2</SUB>O<SUB>3 </SUB>Films Using Binary Reaction Sequence Chemistry", Applied Surface Science (107), 1996, pp. 128-136.
  • Ritala et al.; Perfectly Conformal TiN and Al203 Films Deposited by Atomic Layer Deposition; Chemical Vapor Deposition, v. 5, No. 1, 1999, pp. 7-9.
  • U.S. Appl. No. 09/590,795, filed Jun. 2000, Agarwal et al.
  • U.S. Appl. No. 09/652,532, filed Aug. 31, 2000, Derderian.
  • U.S. Appl. No. 09/653,149, filed Aug. 2000, Derderian.