High impact and wear resistant steel
Abstract
An improved steel railroad rail, and methods for producing same, having a high-carbon content in a range from more than 0.9 to 1.1 wt % is provided that has increased wear resistance and increased fracture toughness over conventional steel rail. The high-carbon rail is characterized as having a pearlitic phase of an eutectoid nature. The average ultimate tensile strength is in a range from 204,860 to 222,120 psi, with a minimum of 174,000 psi. The average yield strength is in a range from 132,320 to 148,450 psi, with the minimum of 120,000 psi. The average percent elongation is in a range from 10.50 to 11.14, with a minimum of 10.00. The Brinell hardness on the surface at any position of the head top and upper gage corners of the rail is in a range from 390 to 440 BHN. The hardness 19 mm below the top surface is in a range from 360 to 435 BHN and 19 mm below the surface at the upper gage corners is in a range from 360 to 410 BHN. The characteristics of the steel rail produced in accordance with the present invention is a substantial improvement as compared with rail used today. The production of a fully pearlitic steel rail having a carbon content from more than 0.9 to 1.1 wt % is
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 16.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for manufacturing a fully pearlitic steel rail of high toughness and high wear resistance, consisting essentially of: forging a steel billet comprising the elements in a range from more than 0.9 to 1 .1 wt % of C, 0.26 to 0.80 by wt % of Si, 0.8 to 1.2 wt % of Mn, less than or equal to 0.35 wt % of Cr, the balance of iron and residual elements; hot rolling the billet to a rolling finishing temperature of about 1000° C. and thereby forming a rail; and cooling the rail at a selected cooling rate in a range from 3.3° C./sec to 4.3° C./sec. beginning substantially at said rolling finishin
- Claim 2Depends on #1
The method according to claim 1 , wherein the steel comprises a maximum of each of the elements 0.45 wt % of Cu, 0.25 wt % of Ni, 0.05 wt % of Mo, 0.025 wt % of S, and 0.01 w
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (1)
- English translation of Japanese patent 1-159327, Hideaki Kageyama, et al, Jun. 22, 1989.