Rapid hardening hydraulic cement from subbituminous fly ash and products thereof
Abstract
A rapid hardening hydraulic cement is provided that is made substantially exclusively from a subbituminous fly ash with no portland cement or other strengthening aid.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 22.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A cement comprising: at least about 85% by weight of a subbituminous fly ash, wherein the subbituminous fly ash comprises a first fly ash that is a class C fly ash and a second fly ash other than a class C fly ash, said second fly ash containing a higher weight fraction of calcium oxide and a higher weight fraction of sulfur trioxide than said first fly ash; less than about 5% by weight of an accelerant; and about 1% to about 10% by weight of at least one alumina-bearing working aid, said cement exhibiting a setting time of about ten minutes or less after mixing with water.
- Claim 2Depends on #1
A cement according to claim 1 , wherein said second fly ash contains more than about 18% calcium oxide and more than about 1.44% sulfur trioxide.
- Claim 3Depends on #1
A cement according to claim 1 , wherein the second fly ash comprises greater than about 5% sulfur trioxide.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 22 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (2)
- Derwent Abstract No. 2000-443201, abstract of Chinese Patent Specification No. 1083406C (Apr. 2002).
- Derwent Abstract No. 2003-854865, abstract of Chinese Patent Specification No. 1442385A (Sep. 2003).