Patents
US 7,282,103 B2#11401722 Most CitedExpiredUnited States (USPTO)Utility

Iron-base amorphous alloy thin strip excellent in soft magnetic properties, iron core manufactured by using said thin strip, and mother alloy for producing rapidly cooled and solidified thin strip

9Forward Citations (#11401722 Global)
0.5/yrCitation Velocity (#17520287 Global)
2.35Citation PageRank (#11219995 Global)
20Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention provides an iron-base amorphous alloy thin strip excellent in soft magnetic properties, an iron core manufactured by using said thin strip, and a mother alloy for producing a rapidly cooled and solidified thin strip. More specifically, the present invention is an iron-base amorphous alloy thin strip produced by rapidly cooling and solidifying molten metal by ejecting it onto a moving cooling substrate through a pouring nozzle having a slot-shaped opening, characterized by having an ultra-thin oxide layer of a thickness in the range from 5 to 20 nm on one or both of the surfaces of the amorphous mother phase containing P in the range from 0.2 to 12 atomic %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 9.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An iron-base amorphous alloy thin strip characterized in that: the composition of said thin strip consists of the main elements of Fe, Si, B, C and one or more of P, As, Bi, S, Se and Te, and further containing one or more of Al, Ti, Zr, V and Nb that form precipitates combining with O, N or C; and the total content of the precipitate forming elements present in the composition of the thin strip is a maximum of 2.5 mass %.

  2. Claim 2Depends on #1

    An iron-base amorphous alloy thin strip according to claim 1 , characterized in that the contents of said main elements are, in atomic percentage, in the ranges from 78 to 86% as to Fe, from 0.02 to less than 4% as to Si, from more than 5 to 16% as to B, from 0.02 to 8% as to C, and from 0.2 to 12% in total as to one or more of P, As, Bi, S, Se and Te.

  3. Claim 3Independent Claim

    An iron-base amorphous alloy

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
JP S57185957 AAmorphous alloy for iron core having high saturated magnetic flux density—20
US 4,504,327 ACorrosion-resistant and wear-resistant magnetic amorphous alloy and a method for preparing the same198519
US 4,588,452 AAmorphous alloys for electromagnetic devices19863
JP S6345318 APartially heat insulated annealing method of amorphous alloy—6
US 4,889,568 AAmorphous alloys for electromagnetic devices cross reference to related applications198913
JP H04329846 AManufacture of fe base amorphous alloy—10
US 5,474,624 AMethod of manufacturing Fe-base soft magnetic alloy199527
JP H08193252 ALow-boron amorphous alloy excellent in soft magnetic property—4
JP H09202946 AIron base amorphous alloy thin strip—14
JP H09202951 AFerrous amorphous alloy for transformer excellent in soft magnetic property and having good workability—4
JP H09268354 ALow boron amorphous alloy excellent in magnetic property and its production—18
JP H11293427 AFerrous amorphous alloy for transformer excellent in soft magnetic property—11
JP H11300450 AFe base amorphous alloy thin band having extremely thin oxidized layer—6
JP 2000054089 AIron-base amorphous alloy excellent in surface characteristic and magnetic property—25
US 6,053,989 AAmorphous and amorphous/microcrystalline metal alloys and methods for their production200041
JP 2000309860 AFe-BASE AMORPHOUS ALLOY RIBBON WITH EXTRA THIN OXIDE LAYER—3
JP 2000313946 AFe-BASE AMORPHOUS ALLOY RIBBON WITH EXTRA THIN OXIDE LAYER—11
US 6,416,879 B1Fe-based amorphous alloy thin strip and core produced using the same200230
JP 2002220646 ARIBBON OF Fe-BASED AMORPHOUS ALLOY AND IRON-CORE MANUFACTURED THEREWITH—8
US 2003205295 A1Low-loss magnetic powder core, and switching power supply, active filter, filter, and amplifying device using the same—18

Non-Patent Literature (3)

  • IEEE Transactions on Magnetics, vol. MAG-11, No. 6, Nov. 1975, pp. 1644-1649.
  • Machine Translation of Japanese Patent Document No. 2000-309860.
  • Morito, Nobuyuki et al. "Degradation of a Small Amount of Ti on the Magnetic Properties of Fe-B-Si Amorphous Alloy" J. Japan Inst. Metals, vol. 52, No. 7 (1988), pp. 733-741.